MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Polyplastics TOPAS® 5013L-10 Cyclic Olefin Copolymer (COC)
Categories: Polymer; Thermoplastic; Cyclo Olefin Polymer

Material Notes: TOPAS® 5013L-10 is a high flow, internally lubricated injection molding grade with a 130°C heat distortion temperature. It is a glass-clear amorphous polymer with outstanding moisture barrier, chemical resistance, high purity and a non-reactive surface making it an excellent choice for healthcare and other high-tech products. This grade has a high heat distortion temperature to withstand 95°C PCR protocols, 121°C steam sterilization protocols, and gamma or EtO procedures.

Key applications and attributes:

  • Labware: Temperature resistant with glass-like clarity; purity
  • Microplates and biochips: Heat and chemical resistant, clarity and purity
  • Microfluidics: Exceptional mold detail replication; machinable
  • Optics: Clarity, low birefringence, low moisture sensitivity
  • Electronics: Low dielectric constant, high flow, thermoplastic
  • Cuvettes: More UV transparent than most resins
  • Healthcare and food: Broad regulatory approval

Information provided by Polyplastics USA, which merged with TOPAS Advanced Polymers in 2018.

Key Words: Polyolefin
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.02 g/cc0.0368 lb/in³ISO 1183
Water Absorption at Saturation 0.010 %
@Temperature 23.0 °C
0.010 %
@Temperature 73.4 °F
ISO 62
Melt Flow 43 g/10 min
@Load 2.16 kg,
Temperature 260 °C
43 g/10 min
@Load 4.76 lb,
Temperature 500 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 46.0 MPa6670 psi5mm/min; ISO 527-2/1A
Elongation at Yield 1.7 %1.7 %5mm/min; ISO 527-2/1A
Tensile Modulus 3.20 GPa464 ksi1mm/min; ISO 527-2/1A
Charpy Impact Unnotched 1.30 J/cm²
@Temperature 23.0 °C
6.19 ft-lb/in²
@Temperature 73.4 °F
ISO 179/1eU
Charpy Impact, Notched 0.160 J/cm²
@Temperature 23.0 °C
0.761 ft-lb/in²
@Temperature 73.4 °F
ISO 179/1eA
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity >= 1.00e+16 ohm-cm>= 1.00e+16 ohm-cmIEC 60093
Dielectric Constant 2.35
@Frequency 1000 - 10000 Hz
2.35
@Frequency 1000 - 10000 Hz
IEC 60250
Comparative Tracking Index >= 600 V>= 600 VIEC 60112
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 127 °C261 °FISO 75-1,-2
Glass Transition Temp, Tg 134 °C273 °F10°C/min; ISO 11357-1,-2,-3
 
Optical PropertiesMetricEnglishComments
Refractive Index 1.5331.533ISO 489
Abbe Number 5656
Transmission, Visible 91.4 %91.4 %ISO 13468-2
 
Processing PropertiesMetricEnglishComments
Feed Temperature <= 100 °C<= 212 °F
Nozzle Temperature 240 - 300 °C464 - 572 °F
Zone 1 230 - 260 °C446 - 500 °F
Zone 2 240 - 270 °C464 - 518 °F
Zone 3 250 - 280 °C482 - 536 °F
Zone 4 260 - 290 °C500 - 554 °F
Mold Temperature 95.0 - 125 °C203 - 257 °F
Injection Velocity 50.0 - 150 mm/sec1.97 - 5.91 in/secModerate to Fast
Injection Pressure 50.0 - 110 MPa7250 - 16000 psiSpecific
Hold Pressure 30.0 - 60.0 MPa4350 - 8700 psiSpecific
Back Pressure <= 15.0 MPa<= 2180 psiSpecific
Screw Speed 50 - 200 rpm50 - 200 rpm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Polyplastics TOPAS® 5013F-04 Cyclic Olefin Copolymer (COC)
Polyplastics TOPAS® 5013S-04 Cyclic Olefin Copolymer (COC)
Polyplastics TOPAS® 8007S-04 Cyclic Olefin Copolymer (COC)
Polyplastics TOPAS® 6013M-07 Cyclic Olefin Copolymer (COC)
Polyplastics TOPAS® 8007X10 Cyclic Olefin Copolymer (COC)

POTOPAS07 / 82421

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.