MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Lord Adhesives Chemlok® 610 Adhesive
Categories: Polymer; Adhesive

Material Notes: Chemlok® 610 is an aqueous adhesive used to bond fluoroelastomers, polyacrylates, ethylene acrylic and peroxide vulcanizing EPDM elastomers. Chemlok 610 aqueous adhesive can also be used as a coating to protect metals against corrosion.

All information provided by Lord.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.9826 g/cc
pH 10 - 14
 
Thermal PropertiesOriginal ValueComments
Flash Point >= 93.0 °CSeta
 
Processing PropertiesOriginal ValueComments
Shelf Life 24.0 Month
@Temperature 21.0 - 27.0 °C
 
Descriptive Properties
AppearanceOrange to Red Liquid
Residue (%)2.5-3.0
SolventsDeionized Water

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PLORD018 / 86026

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.