MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Bohler-Uddeholm UDDEHOLM MIRRAX ESR Plastic Mold Steel
Categories: Metal; Ferrous Metal; Tool Steel; Mold Steel

Material Notes: Uddeholm Mirrax ESR is specially developed and adapted for larger molds that require corrosion resistance and/or high surface finish.

It is characterized by:

  • High hardenability for consistent properties in large dimensions
  • Good ductility and toughness for a safe production
  • High corrosion resistance for low maintenance requirements
  • Excellent polishability for aesthetic quality and function
  • Good wear resistance for longer life
Uddeholm Mirrax ESR is also the right choice for larger tools when contamination in production is totally unacceptable: within the medical industry, optical industry and for other high quality transparent articles.

Applications: Although Uddeholm Mirrax ESR is recommended for all types of moulds, its special properties make it particularly suitable for molds with the following demands:

  • Corrosion/staining resistance, i.e. for moulding of corrosive materials, e.g. PVC, acetates, and for moulds subjected to humid working/storage conditions.
  • High surface finish, i.e. for the production of optical parts, such as camera and sunglass lenses, and for medical components, e.g. syringes, analysis vials etc..
  • Toughness/ductility, i.e. for complex molds
  • Outstanding through-hardening characteristics i.e. high-hardenability, important for larger molds.

Key Words: AISI 420 Modified; W.-Nr. 1.2083
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 7.74 g/cc0.280 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Brinell 250250Annealed
Hardness, Rockwell C 5252without tempering
Tensile Strength, Ultimate 1500 MPa218000 psiat HRC 45
 1780 MPa258000 psiat HRC 50
Tensile Strength, Yield 1200 MPa174000 psiat HRC 45
 1290 MPa187000 psiat HRC 50
Modulus of Elasticity  180 GPa
@Temperature 400 °C
26100 ksi
@Temperature 752 °F
 200 GPa
@Temperature 200 °C
29000 ksi
@Temperature 392 °F
 210 GPa
@Temperature 20.0 °C
30500 ksi
@Temperature 68.0 °F
Impact Test 180 J133 ft-lbwithout tempering; at HRC 52
 220 J162 ft-lbtempered at 300°C; at HRC 50
 
Thermal PropertiesMetricEnglishComments
CTE, linear  11.1 µm/m-°C
@Temperature 20.0 - 200 °C
6.17 µin/in-°F
@Temperature 68.0 - 392 °F
 11.7 µm/m-°C
@Temperature 20.0 - 400 °C
6.50 µin/in-°F
@Temperature 68.0 - 752 °F
Specific Heat Capacity 0.460 J/g-°C0.110 BTU/lb-°F
Thermal Conductivity  20.0 W/m-K
@Temperature 200 °C
139 BTU-in/hr-ft²-°F
@Temperature 392 °F
 24.0 W/m-K
@Temperature 400 °C
167 BTU-in/hr-ft²-°F
@Temperature 752 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
EDRO #8 Premium 420 Stainless Mold Steel
Bohler-Uddeholm UDDEHOLM STAVAX® ESR Modified 420
Crucible Steel CPM® S90V® (420V®) Tool Steel
Bohler-Uddeholm UDDEHOLM STAVAX® SUPREME Modified 420
420 Stainless Steel

NBUCOR44 / 98123

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.