MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Polyram PlusTek PA355M6 Nylon 6.6 for Injection Molding, 30% Mineral Filled, Flame Retardant
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, 30% Mineral Filled

Material Notes: 30% Minerals filled, flame retardant Nylon 6.6 for injection molding applications.

Information provided by Polyram.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.40 g/ccISO 1183
Moisture Absorption at Equilibrium 1.8 %50% RH; ISO 62
Water Absorption at Saturation 5.5 %ISO 62
Linear Mold Shrinkage 0.0080 - 0.012 cm/cmISO 2577
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 118
Tensile Strength, Yield 80.0 MPaISO 527
Elongation at Break 5.0 %ISO 527
Flexural Strength 130 MPaISO 178
Flexural Modulus 4500 MPaISO 178
Izod Impact, Notched (ISO) 5.50 kJ/m²ISO 180
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+15 ohm-cmIEC 60093
Surface Resistance 1.00e+13 ohmIEC 60093
Dielectric Constant 3.7
@Frequency 1e+6 Hz
IEC 60250
Dielectric Strength 85.0 kV/mmIEC 60250
 
Thermal PropertiesOriginal ValueComments
Melting Point 256 °CISO 11357
Maximum Service Temperature, Air 80.0 °CContinuous use
 220 °CShort peaks operation
Deflection Temperature at 0.46 MPa (66 psi) 235 °CISO 75
Deflection Temperature at 1.8 MPa (264 psi) 145 °CISO 75
Flammability, UL94 V-0
@Thickness 3.00 mm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Polyram PlusTek PA350M6 Nylon 6.6 for Injection Molding, 30% Mineral Reinforced
RTP Company RTP 249  Nylon 6/6 (PA 6/6) Mineral 25%
Polyram PlusTek PA352M6 Nylon 6.6, 30% Low Friction Mineral Filled
Akro-Plastic Akromid® C3 GF 30 1 black (4363) PA 6.6/6 Conditioned, Heat Stabilized

PPOLYR839 / 126638

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.