MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Dow ELITE™ 5940G MDPE
Categories: Polymer; Thermoplastic; Polyethylene (PE); Medium Density (MDPE)

Material Notes: Product Description: ELITE™ 5940G Enhanced Polyethylene Resin is a copolymer produced via INSITE™ Technology from Dow. Main Characteristics:
  • MDPE with excellent balance of stiffness and toughness
  • Excellent processability

Availability: North America

Additive: Antiblock: No; Processing Aid: No; Slip: No

Agency Ratings: FDA 21 CFR 177.1520©3.2a; HPFB (Canada) No Objection

Form: Pellets

Information provided by The Dow Chemical Company

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.942 g/ccASTM D792
Melt Flow 0.85 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Puncture Resistance 10.0 lb (f)
Film Tensile Strength at Yield, MD 3000 psiASTM D882
Film Tensile Strength at Yield, TD 3500 psiASTM D882
Film Elongation at Break, MD 460 %ASTM D882
Film Elongation at Break, TD 640 %ASTM D882
1% Secant Modulus 90700 psiMD; ASTM D882
 110000 psiTD; ASTM D882
2% Secant Modulus 73000 psiMD; ASTM D882
 88000 psiTD; ASTM D882
Puncture Energy 17.0 in-lb
Elmendorf Tear Strength MD 40 gASTM D1922
Elmendorf Tear Strength TD 650 gASTM D1922
Dart Drop Test 120 gASTM D1709A
Film Tensile Strength at Break, MD 5200 psiASTM D882
Film Tensile Strength at Break, TD 4700 psiASTM D882
 
Thermal PropertiesOriginal ValueComments
Melting Point 259 °F
Vicat Softening Point 252 °FASTM D1525
 
Optical PropertiesOriginal ValueComments
Haze 30 %ASTM D1003
Gloss 20 %45°; ASTM D2457
 
Processing PropertiesOriginal ValueComments
Melt Temperature 395 °FExtrusion
Blow-up Ratio (BUR) 2.5
 
Descriptive Properties
Film Puncture Resistance115 ft-lb/in3
Film Toughness1300 ft-lb/in3MD, ASTM D882
 1500 ft-lb/in3TD, ASTM D882

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PDOWF501 / 311194

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.