MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Morgan Advanced Ceramics Alsint Porous >99% Alumina
Categories: Ceramic; Oxide; Aluminum Oxide

Material Notes: Exceptional mechanical, thermal, electrical, and chemical properties. High purity grades that can also be used for metallized applications.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 3.75 - 3.95 g/ccFired
Porosity 0.00 %Apparent, fully dense grades
Particle Size 1.0 - 12 µmGrain size
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell 45 N 81 - 86
Vickers Microhardness 14300 - 18500MPa, at Hv 0.5kg
Modulus of Elasticity 370 - 400 GPa
@Temperature 20.0 °C
Flexural Strength 310 - 500 MPa
@Temperature 20.0 °C
3-point
Compressive Strength 2000 - 2500 MPa
Fracture Toughness 4.00 MPa-m½
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+7 - 6.00e+8 ohm-cm
@Temperature 600 °C
 1.00e+14 - 1.00e+17 ohm-cm
@Temperature 20.0 °C
Dielectric Constant 9.3
@Frequency 1e+9 Hz
 9.7 - 10
@Frequency 9.40e+9 Hz
 9.7 - 10.1
@Frequency 1e+6 Hz
Dielectric Strength 20.0 - 31.5 kV/mm
@Thickness 2.00 - 3.00 mm,
Temperature 20.0 °C
DC
Dissipation Factor 0.00014
@Frequency 1e+9 Hz
Dielectric Loss Index 0.00029
@Frequency 1e+7 Hz
K*tan delta
 0.00050 - 0.00080
@Frequency 1e+6 Hz
 0.00050 - 0.0010
@Frequency 9.40e+9 Hz
 0.00084
@Frequency 8.50e+9 Hz
K*tan delta
 0.0013
@Frequency 1e+9 Hz
K*tan delta
 
Thermal PropertiesOriginal ValueComments
CTE, linear 6.90 - 8.90 µm/m-°C
@Temperature 20.0 °C
 8.50 - 9.00 µm/m-°C
@Temperature 800 °C
Specific Heat Capacity 0.880 J/g-°C
Thermal Conductivity 12.5 W/m-K
@Temperature 400 °C
 25.6 - 30.0 W/m-K
@Temperature 20.0 °C
Maximum Service Temperature, Air 1500 - 1725 °C
 
Component Elements PropertiesOriginal ValueComments
Al2O3 >= 99 %
 
Descriptive Properties
Te Value975°C
Thermal Downshock160-210Change in °C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
99.5% Alumina, porous body
Hexcel® HexWeb® CR III 1/16-5052-.0007 Corrosion Resistant Specification Grade Aluminum Honeycomb
Anderman Ceramics EA99P Sintered Alumina, 99%, Porous
Morgan Advanced Ceramics Sintox™ Al (Porous) >99% Alumina
Mitsui HILET™ 1351D Porous Polyethylene Membrane

CMORG22 / 90400

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.