MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Materion eStainless® 300 15/70/15 H2 Temper Stainless/Copper Laminate
Categories: Metal; Nonferrous Metal; Copper Alloy

Material Notes: eStainless steel is a thermally conductive, fully formable clad laminate of stainless steel and copper (SUS/Cu/SUS). It is ideal as a high-conductivity replacement for stainless steel, allowing heat spreading functionality to be designed directly into the structure of devices. Integrated heatsinks made of eStainless clads reduce the need to add specialty thermal management solutions, saving both costs and internal device space. eStainless steels are typically used in consumer electronics devices to enhance the performance of components such as chassis, frames, EMI shields, brackets, and anywhere else that metals are used.

Information provided by Materion.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesOriginal ValueComments
Hardness, Vickers 290 - 350SUS
Tensile Strength, Ultimate 400 MPa
Tensile Strength, Yield 370 MPa
@Strain 0.200 %
Elongation at Break 6.00 %
Flexural Yield Strength 604 - 774 MPa
Flexural Modulus 162 MPa
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.00000200 ohm-cm
 
Thermal PropertiesOriginal ValueComments
Thermal Conductivity 57.0 W/m-KZ
 290 W/m-KX-Y
 
Descriptive Properties
90° Bend Formability<1.0Longitudinal

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

NBB92147 / 323505

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.