MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Refractory Metals

(Viewing data as-entered. Click here to return)
MarkeTech WCu20 Tungsten Copper Alloy  (discontinued **)
Categories: Metal; Nonferrous Metal; Refractory Metal; Tungsten Alloy

Material Notes: Used to fabricate parts to near net size and several processes to produce high quality tungsten based materials.

Tungsten heavy alloys have very high melting point and have a density twice that of steel and are more than 50% heavier than lead. Due to their high density, tungsten alloys offer greater radiation shielding than lead and are non-toxic. Tungsten alloys are electrically and thermal conductive and offer good corrosion resistance. They also have a low coefficient of expansion and have a high modulus of elasticity. Because of these unique properties tungsten alloys are used extensively in military applications, balance weights, aircraft components, nuclear and medical shields, fishing and sport tackle, rocket components, tool vibration dampers, electrical contacts, etc.

Applications:

  • Nuclear and medical radiation shielding for x-ray and shields for radiation therapy and industrial applications.
  • Aircraft and helicopter rotor balance weights
  • Instrument balance weights
  • Weights for sport equipment
  • Tool damping cutter bars
  • High voltage contacts

Data provided by MarkeTech International. MarkeTech International is no longer in business.

Vendors: PLANSEE SE: Whether it's high temperatures, aggressive chemicals or extreme mechanical loading: PLANSEE supplies a suitable product solution in refractory metals or composite materials. As the world market leader in powder metallurgically produced high performance materials we combine outstanding materials knowledge with profound applications and technology know-how. Visit us at www.plansee.com.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 15.2 - 15.6 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Brinell >= 2160HB (MPa)
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity <= 0.00000510 ohm-cm
 
Thermal PropertiesOriginal ValueComments
CTE, linear 8.30 µm/m-°C
@Temperature 20.0 °C
Thermal Conductivity 200 - 220 W/m-K
 
Component Elements PropertiesOriginal ValueComments
Copper, Cu 20 %
Tungsten, W 80 %

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
MarkeTech WCu30 Tungsten Copper Alloy
MarkeTech WCu10 Tungsten Copper Alloy
H.C. Starck WCu 80/20 Tungsten-Copper Composite Material
NAECO® ELKON® R32 Tungsten Copper material ASTM B702
Plansee WCu20 WCuNi

MWAERC1 / 14295

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.