MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Rogers Arlon 51588R019 0.019" (0.483 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate
Categories: Polymer; Thermoset; Silicone; Silicone Rubber; Silicone, Molded, Glass Fiber Filled

Material Notes: Design/Construction:
Side 1: Uncured Silicone Rubber
Substrate: 7628 Style Fiberglass
Side 2, Layer 1: Cured Silicone Rubber
Side 2, Layer 2: Uncured Silicone Rubber
Interleave: Polyethylene

Appearance: Red silicone gum and rubber on fiberglass cloth

This data represents typical values for the production material. The data should not be used to write, or in place of, material specifications.

Information provided by Arlon Silicone Technologies Division; now a part of Rogers Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.34 g/ccSide 1, Silicone Property; Arlon SQA-TMS-024
 1.34 g/ccSide 2, Layer 2, Silicone Property; Arlon SQA-TMS-024
 1.56 g/ccSide 2, Layer 1, Silicone Property; Arlon SQA-TMS-024
Thickness 3.00 milInterleave
 3.50 milSide 1; Arlon SQA-TMS-003
 3.50 milSide 2, Layer 2; Arlon SQA-TMS-003
 4.00 milSide 2, Layer 1; Arlon SQA-TMS-003
 8.00 milSubstrate; Arlon SQA-TMS-003
 19.0 milOverall; Arlon SQA-TMS-003
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 37Side 1, Silicone Property; ASTM D2240
 37Side 2, Layer 2, Silicone Property; ASTM D2240
 55Side 2, Layer 1, Silicone Property; ASTM D2240
Tensile Strength 530 psiSide 2, Layer 1, Silicone Property; ASTM D412
 950 psiSide 1, Silicone Property; ASTM D412
 950 psiSide 2, Layer 2, Silicone Property; ASTM D412
Elongation at Break 300 %Side 2, Layer 1, Silicone Property; ASTM D412
 620 %Side 1, Silicone Property; ASTM D412
 620 %Side 2, Layer 2, Silicone Property; ASTM D412
Tear Strength 40.0 pliSide 2, Layer 1, Silicone Property; ASTM D624
 150 pliSide 1, Silicone Property; ASTM D624
 150 pliSide 2, Layer 2, Silicone Property; ASTM D624
Peel Strength 8.00 pliBond Strength; ASTM D624
 
Electrical PropertiesOriginal ValueComments
Dielectric Strength 728 V/milASTM D149
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 450 °F
Minimum Service Temperature, Air -70.0 °F
Flammability, UL94 HBper card E54153
 
Processing PropertiesOriginal ValueComments
Cure Time 2.00 hour
@Temperature 204 °C
Recommended Postcure Cycle
 15.0 min
@Pressure 0.345 MPa,
Temperature 177 °C
Recommended Cure Cycle
Shelf Life 6.00 Month
@Temperature 23.9 °C
From date of manufacture
 
Descriptive Properties
ColorRed
Total Product Weight (oz/yd2)21.7Arlon SQA-TMS-025

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PARL315 / 125501

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.