Glass reinforced (30 %) - High Temperature Polyamide Alloy, excellent chemical and electrical resistance, high stiffness, modulus and HDT. *All properties are measured after 48 hours of conditioning at 23°C and 50% relative humidity. All samples are prepared according to ASTM standards. Variations within normal tolerances are possible for various types of colors and functional properties like UV resistance. Information provided by Ovation Polymers |