MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
GEHR Plastics ECO-GEHR® WPC-30PP Composite of 70% Wood Fibers and 30% Polypropylene (PP)
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene, Wood Filled

Material Notes: Wood-polymer-composites (WPC) - these materials are composites of standard polymers and wood fibers. The excellent binding of the wood fibers to the polymer gives the materials extremely high mechanical strength. The materials are weather-resistant and can optionally be given anti-bacterial, fungicidal and UV resistant properties.

Information provided by GEHR Plastics, Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.21 g/ccISO 1183
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 75ISO 868
 75ASTM D2240
Tensile Strength at Break 30.0 MPaISO 527
Elongation at Break 1.6 %ISO 527
Modulus of Elasticity 5.18 GPaISO 527
 751 ksiASTM D790
Izod Impact, Unnotched 3.70 ft-lb/inASTM D256
 
Thermal PropertiesOriginal ValueComments
CTE, linear 14.0 µin/in-°FASTM D696
 25.0 µm/m-°CISO 11359
Melting Point 150 °CDIN EN ISO 3146
 302 °FASTM D3418
Maximum Service Temperature, Air 85.0 °CUL 746B
 
Compliance PropertiesOriginal ValueComments
FDA NoPhysiological indifference
 
Descriptive Properties
Bondabilityno
Colornatural
Industrially BiodegradableNo
Physiological indifferenceno, EEC
Renewable Content (%)70
UV Stabilizationno

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
GEHR Plastics ECOGEHR® WPC-30PE Composite of 70% Wood Fibers and 30% Polyethylene (PE)
Akzo Nobel Injection molding of 20% Wood Plastic Composite with 3.25% Expancel 092-120
Lushan 2% WR-2 Wood Plastic Composites Compatibilizer
FKuR Kunststoff Biograde® C 6509 CL Biodegradable Plastic Compound
FKuR Kunststoff Biograde® C 7500 Biodegradable Plastic Compound

PGEHR045 / 122028

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.