MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
EMS-Grivory Grilon® EB 50 H DZ PA6
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6)

Material Notes: Product description: Grilon EB 50 H DZ is a high viscosity, unreinforced, heat stabilized, impact modified PA6 extrusion blow molding grade. Grilon EB 50 H DZ has the following important properties:
  • High melt strength
  • Impact resistant even at low temperatures
  • Good weld line strength
  • Processable on conventional as well as on 3 D-machines
Grilon EB 50 H DZ is used typically for automotive applications such are air ducts for turbo-chargers, air ducts, oil filler pipes, fuel and containers.

Information provided by EMS Grivory.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.10 g/ccDry; ISO 1183
Water Absorption 9.0 %Sim. to ISO 62
Moisture Absorption 3.00 %Sim. to ISO 62
 
Mechanical PropertiesOriginal ValueComments
Ball Indentation Hardness 40.0 MPaConditioned; ISO 2039-1
 100 MPaDry; ISO 2039-1
Tensile Strength, Yield 35.0 MPaConditioned; ISO 527-1/-2
 60.0 MPaDry; ISO 527-1/-2
Elongation at Break 50 %Nominal, Dry; ISO 527-1/-2
 >= 50 %Nominal, Conditioned; ISO 527-1/-2
Elongation at Yield 4.0 %Dry; ISO 527-1/-2
 20 %Conditioned; ISO 527-1/-2
Tensile Modulus 700 MPaConditioned; ISO 527-1/-2
 2300 MPaDry; ISO 527-1/-2
Charpy Impact Unnotched NB
@Temperature 23.0 °C
Conditioned; ISO 179/1eU
 NB
@Temperature -30.0 °C
Conditioned; ISO 179/1eU
 NB
@Temperature 23.0 °C
Dry; ISO 179/1eU
 NB
@Temperature -30.0 °C
Dry; ISO 179/1eU
Charpy Impact, Notched 20.0 kJ/m²
@Temperature -30.0 °C
Dry; ISO 179/1eA
 20.0 kJ/m²
@Temperature -30.0 °C
Conditioned; ISO 179/1eA
 70.0 kJ/m²
@Temperature 23.0 °C
Dry; ISO 179/1eA
 NB
@Temperature 23.0 °C
Conditioned; ISO 179/1eA
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+9 ohm-cmConditioned; IEC 60093
 1.00e+11 ohm-cmDry; IEC 60093
Surface Resistance 1.00e+10 ohmIEC 60093
Dielectric Strength 24.0 kV/mmConditioned; IEC 60243-1
 27.0 kV/mmDry; IEC 60243-1
Comparative Tracking Index 425 VConditioned; IEC 60112
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 120 µm/m-°CISO 11359-1/-2
CTE, linear, Transverse to Flow 140 µm/m-°CISO 11359-1/-2
Melting Point 222 °C10°C/min; ISO 11357-1/-3
Maximum Service Temperature, Air 100 - 120 °CLong Term; ISO 2578
 180 °CShort Term; EMS
Deflection Temperature at 0.46 MPa (66 psi) 90.0 °CISO 75-1/-2
Deflection Temperature at 1.8 MPa (264 psi) 50.0 °CISO 75-1/-2
Flammability, UL94 HBIEC 60695-11-10
 
Descriptive Properties
AutomotiveAir intake systems
 Cooling and climate control
Electricals & ElectronicsCables & Tubes
FormGranules
Industry & Consumer goodsHydraulics & Pneumatics
ProcessingExtrusion - blow molding
 Other Extrusion
Special CharacteristicsImproved heat resistance

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
EMS-Grivory Grilon® EB 50 H PA6
Teknor Apex Chemlon® 275H Nylon 6, Copolymer, Impact Modified
EMS-Grivory Grilon® BRZ 334 H PA6
EMS-Grivory Grilon® BRZ 247 W PA6
EMS-Grivory Grilon® BRZ 234/1 W PA6

PGRH230 / 156939

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.