MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
LyondellBasell Hostacom™ PF062-3 Polypropylene Homopolymer  (discontinued **)
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene with 30% Glass Fiber Filler

Material Notes: Description: Hostacom™ PF062-3 high melt flow, 5,200 MPa flexural modulus, chemically coupled, 30% glass fiber-reinforced polypropylene homopolymer has good impact strength, high stiffness and very good mold filling capability. Uses: Appliances, automotive applications, electrical parts

Information provided by Basell.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 1.12 g/ccASTM D792
Melt Flow 20 g/10 min
@Load 2.16 kg,
Temperature 230 °C
Condition L; ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 13100 psiASTM D 638
Elongation at Yield 2.2 %ASTM D 638
Flexural Yield Strength 20800 psiASTM D790
Flexural Modulus 754000 psiTangent, 0.05 in/min; ASTM D790
Izod Impact, Notched 1.59 ft-lb/in73°F; ASTM D256
Izod Impact, Unnotched 11.1 ft-lb/in73°F; ASTM D256
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 322 °FUnannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 303 °FUnannealed; ASTM D648
UL RTI, Electrical 230 °C
@Thickness 1.59 mm
UL 746
UL RTI, Mechanical with Impact 230 °C
@Thickness 1.59 mm
UL 746
UL RTI, Mechanical without Impact 230 °C
@Thickness 1.59 mm
UL 746
Flammability, UL94 HB
@Thickness 1.59 mm

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
LyondellBasell Higlass PF062-2 Polypropylene Homopolymer, 20% Glass Fiber
LyondellBasell Higlass PF062-4 Polypropylene Homopolymer, 40% Glass Fiber
LyondellBasell Higlass PF072-3 Polypropylene Homopolymer, 30% Glass Fiber
LyondellBasell Pro-fax SV258 Polypropylene Impact Copolymer
LyondellBasell Astryn BC78A Polypropylene Copolymer, 23% Talc

PMO823 / 53812

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.