MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Domo TECHNYL® A 60 G1 V30 PA66, 30% glass fiber, Conditioned
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, 30% Glass Fiber Filled

Material Notes: Description: Flame retardant Polyamide PA66 reinforced with 30% of glass fiber, for injection molding.

Available in: Asia Pacific, Europe, Latin America and North America

Product Applications: This Red Phosphorous and Halogen free flame retardant grade, combines excellent all-round mechanical properties with outstanding flame retardancy (UL 5VA at 1.6mm) and electrical performance. This product is ideally suited for industrial controls and power distribution applications such as MCBs and contactors. The long term thermal performance of this grade also make it ideal for under-the-bonnet Auto applications where it can withstand temperatures of 160°C for over 6000hrs. This product is available in Natural, Grey and Black. Specific colors and Laser Marking grades optimized for YAG and UV laser types are also available upon request.

DOMO Chemicals has acquired Solvay’s Performance Polyamides Business in Europe.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.46 g/ccISO 1183/A
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 115 MPaISO 527 Type 1A
Tensile Modulus 8410 MPaISO 527 Type 1A
Charpy Impact Unnotched 78.0 kJ/m²ISO 179/1eU
Charpy Impact, Notched 9.50 kJ/m²ISO 179/1eA
 
Processing PropertiesOriginal ValueComments
Moisture Content <= 0.20 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Domo TECHNYL® A 60 G1 V25 PA66, 25% glass fiber, DRY
Domo TECHNYL® A 60 G1 V30 PA66, 30% glass fiber, DRY
Domo TECHNYL® A 60 G2 V30 PA66, 30% glass fiber, Conditioned
Domo TECHNYL® A 60 G2 V30 PA66, 30% glass fiber, DRY
Domo TECHNYL® C 236SI PA6, Conditioned

PRHOD725 / 137956

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.