MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Celanese FORTRON 1130L0 PPS, 30% Glass Reinforced
Categories: Polymer; Thermoplastic; Polyphenylene Sulfide (PPS); Polyphenylene Sulfide (PPS) with 30% Glass Fiber Filler

Material Notes: Fortron 1130L0 is a 30% glass-reinforced extrusion grade. It exhibits excellent heat and chemical resistance, good electrical properties and is inherently flame-retardant. The high hardness and rigidity at elevated temperatures allows for good load bearing performance. This product has good weldability due to the modest filler level. 1130L0 is used to produce rods and slabs.

Information provided by Celanese

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Water Absorption 0.020 %
@Temperature 22.8 °C
24hr immersion; ASTM D570
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 160 MPa5mm/min; ISO 527-2/1A
Elongation at Break 2.0 %5mm/min; ISO 527-2/1A
Tensile Modulus 11000 MPa50mm/min; ISO 527-2/1A
Flexural Strength 255 MPaISO 178
Flexural Modulus 10400 MPaISO 178
Izod Impact, Notched (ISO) 9.50 kJ/m²ISO 180/1A
Charpy Impact, Notched 10.0 kJ/m²ISO 179/1eA
 10.0 kJ/m²
@Temperature -30.0 °C
ISO 179/1eA
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+18 ohm-cmIEC 60093
Surface Resistance 1.00e+16 ohmIEC 60093
 
Thermal PropertiesOriginal ValueComments
Melting Point 280 °C10°C/min; ISO 11357-1,-2,-3
Deflection Temperature at 1.8 MPa (264 psi) 255 °CISO 75-1, -2
Glass Transition Temp, Tg 90.0 °CISO 11357-1,-2,-3
Flammability, UL94 V-0
@Thickness 0.380 mm
 
Processing PropertiesOriginal ValueComments
Processing Temperature 140 - 160 °Ccavity
 330 - 340 °Chot runner
Feed Temperature 60.0 - 80.0 °C
Zone 1 290 - 300 °C
Zone 2 310 - 320 °C
Zone 3 330 - 340 °C
Zone 4 330 - 340 °C
Die Temperature 310 - 330 °C
Melt Temperature 310 - 340 °CISO 294
 330 - 340 °C
Mold Temperature 135 - 160 °CISO 294
Drying Temperature 130 - 140 °C
Dry Time 3.00 - 4.00 hour
Moisture Content <= 0.020 %
Injection Pressure 50.0 - 100 MPa
Hold Pressure 30.0 - 70.0 MPa
Back Pressure <= 3.00 MPa
Screw Speed 50 rpm
@Diameter 55.0 mm
 75 rpm
@Diameter 40.0 mm
 120 rpm
@Diameter 25.0 mm
 
Descriptive Properties
Injection moldingNo
Injection speedfast

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Celanese FORTRON 1130L4 PPS, 30% Glass Reinforced
Albis Plastics Tedur® L V 9404-1 PPS, 30% Carbon Fiber
Toyobo TS301 PPS, 30% Glass Fiber Reinforced
Afton Plastics 2300 30% Glass Filled Polyetherimide
Ensinger Tecapeek® CF30 Polyetheretherketone, 30% Carbon Reinforced (PEEK)

PHCQ266 / 178721

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.