MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger SPI

Ensinger TECASINT 5511 SD light-brown Polyimide, Glass Fiber Reinforced
Categories: Polymer; Thermoplastic; Polyimide, Thermoplastic; Thermoplastic Polyimide, Glass Fiber

Material Notes:
  • electrically static dissipative
  • high thermal and mechanical capacity
  • low thermal expansion
  • high creep resistance
  • resistance against high energy radiation
Target Industries:
  • electronics
  • semiconductor technology
  • cryogenic engineering
  • electrical engineering
  • mechanical engineering
  • nuclear and vacuum technology

Information provided by Ensinger Inc.

Vendors: Ensinger High Performance Plastics withstand severe environments, resist harsh chemicals, and perform well in extreme temperatures. They offer weight savings that have potential to drive lower cost systems.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 1.65 g/cc0.0596 lb/in³
Water Absorption 0.60 %
@Time 86400 sec
0.60 %
@Time 24.0 hour
DIN EN ISO 62
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 9292DIN EN ISO 868
Tensile Strength 97.0 MPa14100 psi50 mm/min; DIN EN ISO 527-1
Elongation at Break 2.1 %2.1 %50 mm/min; DIN EN ISO 527-1
Modulus of Elasticity 5.60 GPa812 ksi1 mm/min; DIN EN ISO 527-1
Flexural Strength 128 MPa18600 psi10 mm/min; DIN EN ISO 178
Flexural Modulus 5.588 GPa810.5 ksi2 mm/min; DIN EN ISO 178
Flexural Strain at Break 2.3 %2.3 %10 mm/min; DIN EN ISO 178
Compressive Strain at Break 21.4 %21.4 %10 mm/min; EN ISO 604
Compressive Strength 254 MPa36800 psi10 mm/min; EN ISO 604
Compressive Modulus 5.89 GPa854 ksi1 mm/min; EN ISO 604
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+10 ohm-cm1.00e+10 ohm-cmANSI ESD STM 11.12
Surface Resistance 1.00e+9 - 1.00e+11 ohm1.00e+9 - 1.00e+11 ohmANSI ESD STM 11.11
Surface Resistivity per Square 1.00e+10 - 1.00e+12 ohm1.00e+10 - 1.00e+12 ohmANSI ESD STM 11.11
 
Thermal PropertiesMetricEnglishComments
CTE, linear  32.0 µm/m-°C
@Temperature 23.0 - 100 °C
17.8 µin/in-°F
@Temperature 73.4 - 212 °F
XY; DIN 53 752
 35.0 µm/m-°C
@Temperature 100 - 150 °C
19.4 µin/in-°F
@Temperature 212 - 302 °F
XY; DIN 53 752
 35.0 µm/m-°C
@Temperature 50.0 - 200 °C
19.4 µin/in-°F
@Temperature 122 - 392 °F
XY; DIN 53 752
Specific Heat Capacity 1.01 J/g-°C0.241 BTU/lb-°FDIN EN 821
Thermal Conductivity 0.320 W/m-K
@Temperature 40.0 °C
2.22 BTU-in/hr-ft²-°F
@Temperature 104 °F
DIN EN 821
Maximum Service Temperature, Air 250 °C482 °Flong-term
 300 °C572 °Fshort-term
Minimum Service Temperature, Air -20.0 °C-4.00 °F
Glass Transition Temp, Tg 329 °C624 °FDIN EN ISO 11357
Flammability, UL94 V-0V-0DIN IEC 60695-11-10
 
Descriptive Properties
Colorbrown

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PENSIN8205 / 319133

Chemically Resistant adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.