MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Honeywell A-C® 307 High-density oxidized PE homopolymer
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE)

Material Notes: Hard, high drop point, high density, higher molecular weight (MW), oxidized polyethylene (HDOxPEs) homopolymer in powder form mainly used as a process aid for PVC extrusion. Its low acid number does not allow it be emulsified for use in aqueous systems, like most of Honeywells other high density oxidized polyethylene (HDOxPEs).

Information provided by Honeywell

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.980 g/cc
Brookfield Viscosity 85000 cP
@Temperature 150 °C
 
Chemical PropertiesOriginal ValueComments
Total Acid Number 7.0
 
Thermal PropertiesOriginal ValueComments
Dropping Point 140 °CMettler
 
Descriptive Properties
Hardness<0.5 dmmASTM D5
Product FormGranule

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Global B-8200 High Density Polyethylene
Global F-8000 High Density Polyethylene
Ipiranga Petrochem HC 7260 HDPE
IRPC Polimaxx Polene GA3245 High Density Polyethylene
Celanese GUR® 2122 PE-UHMW, Specialty

PHONWL014 / 179559

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.