MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Industeel FORA 360 BC 360 HB Wear Resistant Steel
Categories: Metal; Ferrous Metal; Carbon Steel; Medium Carbon Steel

Material Notes: Description: FORA 360 BC is a water quenched, abrasion resistant steel, of a hardness 360 HB. It presents at a good aptitude of implementation in particular in welding.

Information provided by manufacturer.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesOriginal ValueComments
Hardness, Brinell 400Typical
Tensile Strength, Ultimate 1200 MPaTypical
Tensile Strength, Yield 1000 MPa
@Strain 0.2 %
Typical
Elongation at Break 14 %Typical, EL 5.65
Charpy Impact 40.0 JTypical (Longitudinal)
 
Component Elements PropertiesOriginal ValueComments
Carbon, C 0.13 %
Chromium, Cr 0.20 %
Iron, Fe 98.29 - 98.32 %As remainder for 16 mm or less plate
Manganese, Mn 1.3 %
Molybdenum, Mo 0.050 %
Phosphorus, P <= 0.020 %
Sulfur, S <= 0.010 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Industeel CREUSABRO® 8000 High Performance Wear Resistant Steel
Industeel CREUSABRO® 4000 High Wear Resistant Steel
Industeel FORA 400 Wear Resistant Steel, 400 HB
Industeel FORA 500 500 HB Wear Resistant Steel
ASTM A36 Steel, plate

NINDUST59 / 17597

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.