MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
317 Stainless Steel, annealed plate
Categories: Metal; Ferrous Metal; Stainless Steel; T 300 Series Stainless Steel

Key Words: UNS S31700, AISI 317, DIN 1.4449, DIN X5CrNiMo1713, ASME SA240, ASME SA249, ASME SA312, ASME SA403, ASME SA409, ASTM A167, ASTM A240, ASTM A249, ASTM A269, ASTM A276, ASTM A312, ASTM A314, ASTM A403, ASTM A409, ASTM A473, ASTM A478, ASTM A511, ASTM A554, ASTM A580, ASTM A632, FED QQ-S-763, SAE J405
Vendors: Visit metalmen for your metals needs. Products include special chemistry, tight tolerances, custom tempers, odd dimensions/forms, and small quantities. Phone 1-800-767-9494.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 8.00 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Brinell 160
Hardness, Knoop 180Converted from Brinell
Hardness, Rockwell B 83
Hardness, Vickers 167Converted from Brinell
Tensile Strength, Ultimate 585 MPa
Tensile Strength, Yield 275 MPa
Elongation at Break 50 %
Modulus of Elasticity 195 GPa
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.0000740 ohm-cmat 20ºC
Magnetic Permeability 1.02approximate value for the annealed condition at RT
 
Thermal PropertiesOriginal ValueComments
CTE, linear 16.0 µm/m-°C
@Temperature 0.000 - 100 °C
 16.2 µm/m-°C
@Temperature 0.000 - 315 °C
 17.5 µm/m-°C
@Temperature 0.000 - 540 °C
Specific Heat Capacity 0.502 J/g-°C
@Temperature 0.000 - 100 °C
Thermal Conductivity 16.3 W/m-K
@Temperature 100 °C
Melting Point 1370 - 1400 °C
Solidus 1370 °C
Liquidus 1400 °C
Maximum Service Temperature, Air 870 °CIntermittent
 925 °CContinuous Service
 
Component Elements PropertiesOriginal ValueComments
Carbon, C <= 0.080 %
Chromium, Cr 18 - 20 %
Iron, Fe 57.85 - 68 %As Balance
Manganese, Mn <= 2.0 %
Molybdenum, Mo 3.0 - 4.0 %
Nickel, Ni 11 - 15 %
Phosphorus, P <= 0.045 %
Silicon, Si <= 1.0 %
Sulfur, S <= 0.030 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
303 Stainless Steel, annealed
AISI Type 317L Stainless Steel, annealed plate
Type 904L Austenitic Stainless Steel, Annealed Plate, Sheet, Strip, UNS N08904
316 Stainless Steel, annealed plate
304 Stainless Steel

MQ317C / 12810

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.