MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
LyondellBasell DP 8310M Polybutene  (discontinued **)
Categories: Polymer; Thermoplastic; Polybutene

Material Notes:
Key Features: semi-crystalline high ethylene content random copolymer

Applications: packaging industry, cast film, FDA acceptable

Meets FDA requirements in 21 CFR 177.1570 for direct food contact up to 212°F (100°C).

Description: Polybutene-1 DP 8310 is a semi-crystalline high ethylene content random copolymer which is miscible with polypropylenes due to its similar moecular structure. In blends with polyethylene it is immiscible but easily dispersible. It is used in the packaging industry as a minor additive in a polyethylene peel seal layer for the production of coextruded glexible film or more rigid sheet. Varying the copolymer concentration in th peel seal layer offers the unique possibility of tailoring the seal strength blown or cast film formulations when imporved optical properties of the reulting fim are required. A typical blend partner is a low density polyethylene iwth a melt index range between 0.5 and 4 dg/min. All other polyethylene types and copolymers of the same melt index range can be used. It can also be used in blends wiht polypropylenes to reduce flexural modulus and hardness characteristics very effectively. This resin meets FDA requirements for direct food contact at temperatures up to 100°C under regulation 21 CFR 177.1570.

Information provided by Montell Polyolefins.

LyondellBasell is the successor company to Montell.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.895 g/ccASTM D1505
Melt Flow 3.0 g/10 minISO 1133-1981E
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Ultimate 24.1 MPaISO 1184-1983E
Tensile Strength, Yield 3.74 MPaISO 1184-1983E
Elongation at Break 550 %ISO 1184-1983E
Modulus of Elasticity 0.0517 GPaISO 1184-1983E
 
Thermal PropertiesOriginal ValueComments
Melting Point 116 °CDSC
Vicat Softening Point 90.0 °CASTM D1525
Brittleness Temperature -34.0 °CASTM D746
 
Compliance PropertiesOriginal ValueComments
FDA YesSee notes for details.

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Polybutadiene Rubber (BR)
LyondellBasell Montell 8340 Polybutene-1
LyondellBasell Montell 0800 Polybutene
LyondellBasell Montell 0300 Polybutene
LyondellBasell DP 8510M Polybutene

PMO714 / 53727

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.