MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Evonik SIPERNAT® 50 Silica Powder
Categories: Other Engineering Material

Material Notes: Properties and applications: SIPERNAT represents a specific product range of precipitated silica, aluminum and calcium silicates. As a carrier silica with particularly high absorbency, SIPERNAT 50 has the capacity to convert liquid active substances or solution into powders. Concentrates of up to 75 percent can be produced using SIPERNAT 50. It is also used as a grinding aid for fatty products. Typical applications include:
  • rubber and plastics additives
  • plant protection formulations
  • feed additives
  • carrier for powder defoamer

Information provided by Evonik

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.180 g/ccTamped; ISO 787-11
Particle Size 50 µmd50; ISO 13320-1
pH 6.05% in water; ISO 787-9
Specific Surface Area 500 m²/gISO 9277
 
Component Elements PropertiesOriginal ValueComments
SiO2 >= 97 %ISO 3262-19
Sodium, Na <= 0.60 %
 
Descriptive Properties
Content<1.0%Sulfate
 <400 ppmIron

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Evonik BREAK-THRU® AF 9908 Surfactants
Evonik SIPERNAT® 383 DS Silica Powder
Evonik SIPERNAT® 35 Silica Powder
Evonik SIPERNAT® 320 DS Silica Powder
Evonik SIPERNAT® 160 Ceramic Powder

PEVONIM044 / 197248

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.