MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Envalior Stanyl® TE341 Nylon 46 (European Grade) (Dry)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 46 (PA46); Nylon 46, Unreinforced

Material Notes: Stanyl is a high performance polyamide providing good performance and value across a broad range of automotive and electronic applications. Stanyl offers:
  • Highest mechanical properties at high temperatures
  • Excellent resistance to wear and low friction
  • Outstanding flow for easy processing and exceptional design freedom
  • Stanyl High Flowgrades that match the best flowing LCPs while maintaining a high level of mechanical properties

Key Applications:

  • Automotive: Powertrain components, Charge-air coolers, EPS and ETC gears, Motor Sensors, Auto connectors, Chain tensioners
  • E&E: Connectors, Microswitches, Bobbins, Memory modules, Motor components, Industrial, Specialty films and fibers, Consumer appliances

    Information provided by DSM.

    Former DSM Engineering Plastics product line is now with Envalior.

  • Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
     
    Physical PropertiesMetricEnglishComments
    Density 1.18 g/cc0.0426 lb/in³ISO 1183
    Water Absorption 13 %13 %Sim. to ISO 62
    Moisture Absorption at Equilibrium 3.7 %3.7 %Humidity Absorption; Sim. to ISO 62
    Viscosity Number 185 cm³/g1.85 dl/g
    Linear Mold Shrinkage, Flow 0.020 cm/cm0.020 in/inISO 294-4
    Linear Mold Shrinkage, Transverse 0.020 cm/cm0.020 in/inISO 294-4
     
    Mechanical PropertiesMetricEnglishComments
    Tensile Strength, Yield 100 MPa14500 psiISO 527-1/-2
    Elongation at Break 40 %40 %ISO 527-1/-2
    Elongation at Yield 10 %10 %ISO 527-1/-2
    Tensile Modulus 3.30 GPa479 ksiISO 527-1/-2
    Charpy Impact Unnotched  NB
    @Temperature -30.0 °C
    NB
    @Temperature -22.0 °F
    ISO 179/1eU
     NB
    @Temperature 23.0 °C
    NB
    @Temperature 73.4 °F
    ISO 179/1eU
    Charpy Impact, Notched  0.900 J/cm²
    @Temperature -30.0 °C
    4.28 ft-lb/in²
    @Temperature -22.0 °F
    ISO 179/1eA
     1.20 J/cm²
    @Temperature 23.0 °C
    5.71 ft-lb/in²
    @Temperature 73.4 °F
    ISO 179/1eA
     
    Electrical PropertiesMetricEnglishComments
    Comparative Tracking Index 600 V600 VIEC 60112
     >= 600 V>= 600 VPLC 0; UL 746A
     
    Thermal PropertiesMetricEnglishComments
    CTE, linear, Parallel to Flow 80.0 µm/m-°C
    @Temperature 20.0 °C
    44.4 µin/in-°F
    @Temperature 68.0 °F
    ISO 11359-1/-2
    CTE, linear, Transverse to Flow 100 µm/m-°C
    @Temperature 20.0 °C
    55.6 µin/in-°F
    @Temperature 68.0 °F
    ISO 11359-1/-2
    Melting Point 295 °C563 °F10°C/min; ISO 11357-1/-3
    Deflection Temperature at 0.46 MPa (66 psi) 280 °C536 °FISO 75-1/-2
    Deflection Temperature at 1.8 MPa (264 psi) 190 °C374 °FISO 75-1/-2
    Vicat Softening Point 290 °C554 °F50°C/h 50N; ISO 306
    Glass Transition Temp, Tg 75.0 °C167 °FGlass Transition Temperature (10°C/min); ISO 11357-1/-2
    UL RTI, Electrical  130 °C
    @Thickness 1.50 mm
    266 °F
    @Thickness 0.0591 in
    UL746B
     130 °C
    @Thickness 0.750 mm
    266 °F
    @Thickness 0.0295 in
    UL746B
    Flammability, UL94  V-2
    @Thickness 0.750 mm
    V-2
    @Thickness 0.0295 in
    IEC 60695-11-10
     V-2
    @Thickness 1.60 mm
    V-2
    @Thickness 0.0630 in
    IEC 60695-11-10
     
    Descriptive Properties
    Heat Stabilized or Stable to HeatYes
    Injection MoldingYes
    LubricantsYes
    Release AgentYes
    Without FillersYes

    Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

    Users viewing this material also viewed the following:
    Envalior Stanyl® TW441 Nylon 46 (European and Asian Grade) (Cond)
    BASF Elastollan® C-90A Polyester Type Polyurethane Elastomer
    BASF Elastollan® C-85A Polyester Type Polyurethane Elastomer
    BASF Elastollan® 1174D Polyether Type Polyurethane Elastomer
    Asahi Kasei Leona™ 14G25 Polyamide 66, Heat Stabilized, GF Reinforced

    PDSMEU478 / 31360

    Aluminum Castings

    Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

    The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.