MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Arkema Rilsan® BESN BLACK P20 TL Nylon 11, Flexible Tubing Grade
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 11 (PA11); Nylon 11, Flexible Tubing Grade

Material Notes: Designation ISO 1874-PA11-P,EHL,22-004

Flexible grade for tubes extrusion. Available color: black and natural. Light and heat stabilized.

Flexibility. High impact strength. Very good chemical resistance. Ability to be processed at high speed.

Example applications: Flexible tubes for automotive.

Information provided by Arkema.

Key Words: PA11; Polyamide 11
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.04 g/ccISO 1183
 1.04 g/ccCond.; ISO 1183
Water Absorption 1.8 %Dry; Sim. to ISO 62
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 32.0 MPaCond.; ISO 527-1/-2
Elongation at Break >= 50 %Cond.; ISO 527-1/-2
Elongation at Yield 33 %Cond.; ISO 527-1/-2
Tensile Modulus 560 MPaCond.; ISO 527-1/-2
Charpy Impact Unnotched NB
@Temperature -30.0 °C
Cond.; ISO 179/1eU
 NB
@Temperature 23.0 °C
Cond.; ISO 179/1eU
Charpy Impact, Notched 10.0 kJ/m²
@Temperature -30.0 °C
Cond.; ISO 179/1eA
 70.0 kJ/m²
@Temperature 23.0 °C
Cond.; ISO 179/1eA
 
Thermal PropertiesOriginal ValueComments
Melting Point 182 °C10°C/min; Dry; ISO 11357-1/-3
Deflection Temperature at 0.46 MPa (66 psi) 135 °CDry; ISO 75-1/-2
Deflection Temperature at 1.8 MPa (264 psi) 47.0 °CDry; ISO 75-1/-2
 
Processing PropertiesOriginal ValueComments
Melt Temperature 270 °CInjection Molding; ISO 294
Mold Temperature 50.0 °CInjection Molding; ISO 10724
Hold Pressure 16.0 MPaInjection Molding; ISO 294
 
Descriptive Properties
%Bio-Based92ASTM D6866
Bio-BasedYes
Form as DeliveredPellets
Heat StabilizedYes
Light StabilizedYes
LubricantsYes
Moisture SensitiveYes
PlasticizerYes
Processing MethodsInjection Molding
 Other Extrusion
 Profile Extrusion

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Arkema Rilsan® BESNO P20 TL PA11
Arkema Rilsan® BESN BLACK P40 TL Nylon 11, Flexible Tubing Grade
Arkema Rilsan® BESN BLACK TL Nylon 11, Rigid Tubing Grade
Arkema Rilsan® BESVO A FDA Nylon 11
Arkema Rilsan® 8020 Nylon 11, Flexible Tubing Grade

PARKG616 / 25868

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.