MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Saint-Gobain Chemfab® TCN® 2000 High-Strength Leno Weave Nomex/Fiberglass Belting Material
Categories: Ceramic; Glass; Glass Fiber

Material Notes: Description: General Notes on Saint Gobain Chemfab® TCN® Open Mesh Belting Products:
TCN belting products are PTFE coated Nomex®, a high-temperature polyamide fiber that maintains its structural integrity over its entire range of operating temperatures. These belts were developed for applications requiring continuous operation, outstanding tracking and predictable dimensional stability. TCN will not shrink or stretch--not even by 2%--under normal operating tensions.
Dimensional Stability: Width rigidity as well as length stability is maintained by TCN belting in continuous use at temperatures up to 500°F. Under normal operating tensions (3 to 10 pounds per inch of width), TCN holds its elongation and shrinkage to less than 2%.
Release Properties: The release properties of TCN equal or exceed those of any other available belting material. The PTFE makes TCN have a low coefficient of friction.
Chemically Resistant: The PTFE coating encapsulates the Nomex® belting carcass and enhances its useful service life.
Dynamic Strength: TCN has durability coupled with low overall belt weight, allowing optimal production speed with decreased power requirements.
Flex Fatigue Resistant: The flex fatigue resistance of Nomex--the lengthwise strength yarn in TCN belting--is designed for high temperature use. This flex fatigue resistance is maintained throughout the entire operating range of TCN belting.
Temperature Resistant: TCN belting can be operated continuously at temperatures up to 500°F and will still maintain 100% of its operational profile.
Low Thermal Mass: TCN belting (including the seam areas) quickly dissipates heat with low heat sink properties.
Fabrication Technology: Saint-Gobain Performance Plastics belt seams have been specifically engineered to reduce the flex fatigue failure. Substantially reduced flex fatigue means longer belt life.
Specific Notes on TCN® 2000 Belting Material: TCN 2000 is an open mesh, Leno weave belting material designed for use in forced hot air dryers. The warp yarns are Nomex®, which allows the belt to conform to machine irregularities. The filling yarn is extra heavy for maximum stiffness in the cross-machine direction. The substrate is Leno weave, with Nomex® in the warp/longitudinal direction and fiberglass in the fill/transverse direction. The substrate is coated in PTFE (PTFE = polytetrafluoroethylene). All data based on a 0.085 inch test sample.
Information provided by Saint Gobain Performance Products.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 32.35 - 37.25 lb/ft³
 
Mechanical PropertiesOriginal ValueComments
Elongation at Yield <= 2.0 %Value given for Elongation at a loading of 40 lbs/in
Tear Strength 150 pliTensile Strength (Warp)
 700 pliTensile Strength (Fill)
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 500 °F
 
Descriptive Properties
Weight (oz/yd^2)37

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Saint-Gobain Chemfab® TCN® 1590 Leno Weave Nomex/Fiberglass Belting Material
Rogers Arlon 51112R013 0.013" (0.330 mm) Cured, Self Fusing, Silicone Rubber with Fiberglass Substrate
DuPont™ Nomex® 430 1200 Denier Aramid Yarn
Solvay 200TFNP PTFE-coated fiberglass cloth
Saint-Gobain COHRlastic® 300AR Reinforced Silicone Sponge/Aggressive Acrylic Adhesive Pressure Sensitive Tape

CSTGQZ128 / 2257

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.