MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Performance Alloys MoldStar® 90 Copper Mold Alloy
Categories: Metal; Nonferrous Metal; Copper Alloy

Material Notes: Description: MoldStar® 90 is a beryllium-free copper alloy for the blow molding and injection molding industries as well as other industrial applications. MoldStar® 90 provides a good balance of thermal conductivity, hardness, corrosion resistance and wear.

Applications:

  • Mold Inserts
  • Thermal Pins
  • Mold Cores
  • Cavities
  • Lifters
  • Etc.

Information provided by Performance Alloys.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.310 lb/in³
 
Mechanical PropertiesOriginal ValueComments
Hardness, Brinell 3113000kg
Hardness, Rockwell C 31
Tensile Strength at Break 150000 psi
Tensile Strength, Yield 140 ksi
Elongation at Break 5.0 %in 2"
Compressive Strength 140 ksi
 
Thermal PropertiesOriginal ValueComments
CTE, linear 9.50 µin/in-°F
@Temperature 20.0 °C
Thermal Conductivity 1080 BTU-in/hr-ft²-°F
@Temperature 15.6 °C
 
Component Elements PropertiesOriginal ValueComments
Copper, Cu 89 %
Nickel, Ni 7.5 %
Other 3.5 %
 
Descriptive Properties
Thermal diffusivity at 68°F1.76 ft²/hr

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Performance Alloys MoldStar® 150 (PAS 940) Copper Mold Alloy
Ampco Metal AMPCO® 45 Nickel-Aluminum Bronze, Extruded and Drawn Rods, 25.4 - 50.8 mm.
Ampco Metal AMPCOLOY® 940 Nickel-Copper, Extrusion, ≤ 25 mm.
Ampco Metal AMPCOLOY® 940 Nickel-Copper, Extrusion, > 50 mm.
Ampco Metal AMPCOLOY® 940 Nickel-Copper, Extrusion, 25 - 50 mm.

NPER01 / 18768

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.