MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

USP Class VI Adhesives
USP Class VI Approved Adhesives for Medical Device Applications
Master Bond’s biocompatible adhesives are designed to meet the needs of medical device manufacturers. Compounds withstand various types of sterilization methods.

(Viewing data as-entered. Click here to return)
Celanese 7110 LDPE polymer for medical
Categories: Polymer; Thermoplastic; Polyethylene (PE); Low Density (LDPE); Low Density Polyethylene (LDPE), Molded

Material Notes: 7110 is a high strength polyethylene resin designed for the blow molding of small containers and vials, and manufactured to comply with USP Class VI. This LDPE resin may be safely used as articles or components of articles intended for uses in contact with food as provided in FDA regulation 21 CFR 177.1520 - Polyethylene, subject to extraction limitations on the finished food-contact article as specified in that regulation. Additives:

Applications: Medical Packaging

Information provided by Celanese Corporation.

Key Words: blow molding of small containers and vials
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.922 g/ccAT Plastics PTM-03
Melt Flow 0.80 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 52ASTM D2240
Tensile Strength at Break 20.0 MPaType IV (50 mm/min); ASTM D638
Elongation at Break 600 %Type IV (50 mm/min); ASTM D638
Flexural Modulus, 1% Secant 0.269 GPaASTM D790
 
Thermal PropertiesOriginal ValueComments
Melting Point 114 °CDSC; ASTM D3417
Vicat Softening Point 99.6 °CASTM D1525
 
Compliance PropertiesOriginal ValueComments
FDA YesSee notes for details.
USP Class VI Yes

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Dow ATTANE™ 4701 Ultra Low Density Polyethylene, Medical Packaging Grade
Dow ATTANE™ 4601 Ultra Low Density Polyethylene, Medical Packaging Grade
LyondellBasell Montell 1900 UHMW Polyethylene
Chevron Phillips HiD® 99416 with Food Grade Antistat HDPE Blow Molding Resin
Braskem HB0454HR HDPE Blow Molding Polyethylene Copolymer

PATEVB73 / 26029

USP Class VI Adhesives
USP Class VI Approved Adhesives for Medical Device Applications
Master Bond’s biocompatible adhesives are designed to meet the needs of medical device manufacturers. Compounds withstand various types of sterilization methods.

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.