MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Lotte Advanced Materials Starex® TX-0520T Transparent Grade ABS
Categories: Polymer; Thermoplastic; ABS Polymer; Acrylonitrile Butadiene Styrene (ABS), Transparent, Molded

Material Notes: Information provided by Polymer Technology and Services, LLC (PTS).

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.10 g/ccASTM D792
Linear Mold Shrinkage 0.0040 - 0.0070 cm/cmASTM D955
Melt Flow 16 g/10 min
@Load 10.0 kg,
Temperature 220 °C
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 6254 psi
@Thickness 3.17 mm
Elongation at Break 14 %
@Thickness 3.17 mm
ASTM D638
Flexural Strength 8528 psi
@Thickness 3.17 mm
ASTM D790
Flexural Modulus 280000 psi
@Thickness 3.17 mm
ASTM D790
Izod Impact, Notched 2.75 ft-lb/in
@Thickness 3.17 mm
ASTM D256
 
Thermal PropertiesOriginal ValueComments
Flammability, UL94 HB
@Thickness 1.50 mm
 
Optical PropertiesOriginal ValueComments
Haze 2.7 %ASTM D1003
Transmission, Visible 89 %ASTM D1003
 
Processing PropertiesOriginal ValueComments
Melt Temperature 374 - 446 °FInjection Temp
Mold Temperature 104 - 176 °F
Drying Temperature 167 - 176 °F
Dry Time 2 - 4 hour
Injection Pressure 9940 - 15620 psi
Back Pressure 142 - 284 psi
Screw Speed 60 - 90 rpm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
LG Chemical TR556 MABS, Transparency, Chemical Resistance
LG Chemical TR300 MABS, Flame Retardant, Transparency
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Transparent, Molded
Covestro Makrolon® 2458 Polycarbonate, Injection Grade
Covestro Apec® 1745 Polycarbonate

PLBST000a / 146084

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.