MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Evonik DYNAPOL® S 1401 Linear Copolyester
Categories: Polymer; Thermoplastic; Polyester, TP

Material Notes: A saturated, linear copolyester, slightly crystalline. Generally used in a solution, film or melt from heated tanks or extruders for the adhesion of aluminum, PET, PVC, ABS, copper, paper, cardboard, leather and fabric

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.20 g/ccDIN 53 479
Viscosity 15000 cP
@Temperature 220 °C
melt; (Plate/Plate)
 25000 cP
@Temperature 200 °C
melt; (Plate/Plate)
 40000 cP
@Temperature 180 °C
melt; (Plate/Plate)
 80000 cP
@Temperature 160 °C
melt; (Plate/Plate)
Viscosity Test 75 - 85 cm³/gDIN 53 728
Melt Flow 110 g/10 min
@Temperature 160 °C
DIN ISO 1133
 190 g/10 min
@Temperature 180 °C
DIN ISO 1133
 290 g/10 min
@Temperature 200 °C
DIN ISO 1133
 
Chemical PropertiesOriginal ValueComments
Total Acid Number <= 3.0DIN EN ISO 2114
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 19
Tensile Strength, Ultimate 5.00 MPaDIN EN ISO 527-1/3
Elongation at Break 800 %
 
Thermal PropertiesOriginal ValueComments
Melting Point 80.0 - 95.0 °Coptical; Mettler FP 82
Softening Point 100 °CDIN ISO 4625
Glass Transition Temp, Tg -25.0 °CDIN 53 765
 
Descriptive Properties
Hydroxyl Number (mg KOH/g)4-10DIN 53 240-2

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
EMS-Griltech Griltex® D 1619E Copolyester Hotmelt Adhesive (Technical Applications)
EMS-Griltech Griltex® D 1616E Copolyester Hotmelt Adhesive (Technical Applications)
EMS-Griltech Griltex® D 1365E Copolyester Hotmelt Adhesive (Technical Applications)
EMS-Griltech Griltex® D 1582E Copolyester Hotmelt Adhesive (Technical Applications)
EMS-Griltech Griltex® D 1655E Copolyester Hotmelt Adhesive (Technical Applications)

PHUMB267 / 81269

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.