MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Greene Tweed CHEMRAZ® 522 Perfluoroelastomer
Categories: Polymer; Thermoset; Fluoropolymer, TS; Thermoset Fluoroelastomer; Rubber or Thermoset Elastomer (TSE)

Material Notes: Chemraz®, a proprietary Greene, Tweed compound, has the broadest chemical resistance of any elastomeric material. Chemraz combines the resilience and sealing force of an elastomer with chemical resistance approaching that of PTFE. Chemraz designs last longer and seal better in harsh environments at a wider range of temperatures than any other elastomer on the market. Chemraz solves some of the most difficult sealing problems encountered in many industries while delivering outstanding in-use cost effectiveness through custom components.

Information provided by Greene Tweed.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.88 g/ccASTM D297
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 95ASTM D2240
Tensile Strength at Break 1500 psiASTM D1414
Elongation at Break 28 %ASTM D1414
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 400 °F
Minimum Service Temperature, Air 0.000 °F
 
Descriptive Properties
ColorBlack

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
DuPont Mobility and Materials Kalrez® 6375UP FFKM Perfluoroelastomer
DuPont Mobility and Materials Kalrez® 6375 FFKM Perfluoroelastomer
DuPont Mobility and Materials Kalrez® 6230 FFKM Perfluoroelastomer
DuPont Mobility and Materials Kalrez® 6221 FFKM Perfluoroelastomer
DuPont Mobility and Materials Kalrez® 4079AMS FFKM Perfluoroelastomer

PGREEN07 / 42301

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.