MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Syensqo (Solvay Specialty Polymers) Polidan® T/A-SL Polyethylene, Crosslinked (XLPE)  (discontinued **)
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE); High Density Polyethylene (HDPE), Crosslinkable (XLPE)

Material Notes: POLIDAN® T/A-SL is a silane crosslinkable PE compound which is used together with a catalyst masterbatch to accelerate the crosslinking reaction. It is used for flexible crosslinkable pipes. Applications - POLIDAN® T/A-SL is used for the production of pipes for domestic hot and cold water supply. This compound is designed for both mono layer and composite pipe solutions.

Additional Information: Above values are typical averages obtained from 18 x 2 mm mono layer pipe specimens which are extruded with 95 parts of POLIDAN® T/A-SL and 5 parts of CATALYST PS/2 or PS/4. These pipe specimens are cured by immersion in 95°C hot water for 6 hours. Storage and Handling - In order to avoid pre-mature crosslinking, the silane crosslinkable compound and the catalyst masterbatch shall be stored separately and mixed only when used. The silane crosslinkable compound shall be used within 6 - 8 hours after bags are opened. - The product shall be stored under the following conditions: -- Closed and unbroken bags -- Ambient temperature not exceeding 40°C -- Indoor in order to avoid direct exposure to sunlight - The product could undergo alterations due to extended period of storage. Solvay Specialty Polymers suggests the product use within six months from the production date printed on the packaging. Solvay Specialty Polymers accepts no liability of any kind in case the above mentioned conditions are not fulfilled. Packaging - POLIDAN® T/A-SL is supplied in 500 kg octabins which contain a single moisture resistant bag or in 25 kg moisture resistant bags placed on 1375 kg pallets. Technical Service - POLIDAN® T/A-SL is part of the Solvay Specialty Polymers POLIDAN® PEX System product range. Solvay Specialty Polymers Technical Service is available to assist customers with further information and advice including the start-up and also for any eventual necessity during the use of the product.

Extrusion Notes: Processing Guidelines - The silane crosslinkable compound POLIDAN® T/A-SL shall be used together with a Solvay Specialty Polymers catalyst masterbatch in the ratio of 95 to 5 parts respectively. Mixing shall be done just before extrusion or during the extrusion process with the use of automatic feeders. POLIDAN® T/A-SL can be processed with modern PE single screw extruders. Curing - The final pipe properties are curing dependent. - Curing can be done in the following ways: -- by immersion in hot water at 90-95°C -- by circulation of hot water inside the pipe at 90-95°C -- by exposure to steam - In all cases curing time depends on the pipe wall thickness, pipe structure and applied curing temperature. Colouring - POLIDAN® compounds and catalyst masterbatches can be used together with good quality PE based colour masterbatches. Solvay Specialty Polymers suggests pre-drying all colour masterbatches prior to use.

Information provided by Solvay Specialty Polymers.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.949 g/ccASTM D792
Melt Flow 0.60 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ISO 1133
 2.4 g/10 min
@Load 5.00 kg,
Temperature 190 °C
ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength >= 20.0 MPaASTM D638
Elongation at Break >= 400 %ASTM D638
Tensile Modulus 670 MPa
@Temperature 23.0 °C
ISO 527-2
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 160 µm/m-°C
@Temperature 20.0 °C
ASTM D696
Specific Heat Capacity 1.80 J/g-°C
@Temperature 23.0 °C
ISO 11357
Thermal Conductivity 0.470 - 0.490 W/m-K
@Temperature 23.0 °C
Hot disk method; Internal Method
Vicat Softening Point 127 °CASTM D1525
 
Processing PropertiesOriginal ValueComments
Zone 1 150 - 200 °C
Zone 2 150 - 200 °C
Zone 3 150 - 200 °C
Zone 4 150 - 200 °C
Zone 5 150 - 200 °C
Die Temperature 210 °C
Head Temperature 200 °C
 
Descriptive Properties
Agency RatingsISO 15875 /2
AvailabilityAsia Pacific
 Europe
 North America
Extruder Screw Compression Ratio>2.5:1
Extruder Screw L/D Ratio25:1 to 30:1
FeaturesCrosslinkable
 Good Processing Stability
 High Density
Gel Content> 65% EN579Crosslinking level
GenericXLPE
Processing MethodExtrusion
 Pipe Extrusion
UsesPiping
 Plumbing Parts
 Potable Water Applications

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
LyondellBasell Aquathene® FR409800 Polyethylene Wire and Cable Compound
Syensqo (Solvay Specialty Polymers) Polidan® T/A-MD Polyethylene, Crosslinked (XLPE)
A. Schulman SCHULINK® X XL350 Cross-Linkable, High Density Polyethylene
Syensqo (Solvay Specialty Polymers) Polidan® EC/110 Polyethylene, Crosslinked (XLPE)
Syensqo (Solvay Specialty Polymers) Polidan® PNT 0553/23 Polyethylene, Crosslinked (XLPE)

PSOL8Y7727 / 135786

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.