MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Borealis Nepol™ GB601HP Polypropylene, 30% Long Glass Fiber Reinforced w/BJ356MO  (discontinued **)
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene with 30% Glass Fiber Filler

Material Notes: Nepol™ GB601HP is a special long glass fiber reinforced polypropylene concentrate grade intended for injection molding and extrusion. This material is designed for the dilution process in combination with special developed dilution polypropylene grades, preferably homopolymer HK060AE or copolymer BJ356MO. This combination of concentrate- dilution polypropylene should be then adjusted for a glass fiber content range of 20-40% in the end product. Applications: Electrical components, load bearing automotive parts, force transmission parts, front end carriers, dashboard carriers and door module carriers.

Information provided by Borealis AG

Key Words: PP
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Filler Content 30 %30 %
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 120 MPa17400 psiISO 527-2
Elongation at Break 2.3 %2.3 %ISO 527-2
Tensile Modulus 7.40 GPa1070 ksiISO 527-2
Flexural Strength 160 MPa23200 psi3.1% strain; ISO 178
Flexural Modulus 6.90 GPa1000 ksiISO 178
Charpy Impact Unnotched  4.50 J/cm²
@Temperature 23.0 °C
21.4 ft-lb/in²
@Temperature 73.4 °F
ISO 179/1fU
 5.50 J/cm²
@Temperature -30.0 °C
26.2 ft-lb/in²
@Temperature -22.0 °F
ISO 179/1fU
 5.60 J/cm²
@Temperature 23.0 °C
26.6 ft-lb/in²
@Temperature 73.4 °F
ISO 179/1eU
Charpy Impact, Notched 1.80 J/cm²
@Temperature 23.0 °C
8.57 ft-lb/in²
@Temperature 73.4 °F
ISO 179/1eA
Dart Drop, Total Energy 14.5 J
@Temperature 23.0 °C
10.7 ft-lb
@Temperature 73.4 °F
3500N, 6.2mm deflection; ISO 6603
 
Processing PropertiesMetricEnglishComments
Feed Temperature 220 - 240 °C428 - 464 °F
Melt Temperature 240 - 270 °C464 - 518 °F
Mold Temperature 60.0 - 100 °C140 - 212 °F
Injection Velocity 20.0 - 30.0 mm/sec0.787 - 1.18 in/sec
Injection Pressure 30.0 - 60.0 MPa4350 - 8700 psi
Screw Speed 30 - 150 rpm30 - 150 rpm
 
Descriptive Properties
Back Pressure0-10% of injection pressure
Hold Pressure50-70% of injection pressure

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Adell RR-16 Copolymer Polypropylene, 30% Glass Reinforced
A. Schulman POLYFLAM™ E-14526-31 30% Glass Reinforced Chemically Coupled Polypropylene
Borealis Nepol™ GB601HP Polypropylene, 40% Long Glass Fiber Reinforced w/BJ356MO
Borealis Xmod™ HF006SA High Stiffness Polypropylene for Injection Molding Applications
Overview of materials for Polypropylene with 30% Glass Fiber Filler

PBOREA548 / 108807

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.