MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Aremco

(Viewing data as-entered. Click here to return)
Aremco Pyro-Putty™ 950 High Temperature Ceramic-Metallic Putty, Ceramic Fiber Filled
Categories: Ceramic; High Temp Ceramic Resin

Material Notes: Pyro-Putty® High Temperature Pastes are used to seal joints and repair defects in cast aluminum, cast iron, steel and stainless steel. Formulated using the most advanced organic and inorganic-ceramic technologies, these materials resist temperatures to over 2000°F. Applications for Pyro-Putty® are widespread and found typically in the aerospace, automotive, foundry, heat treating, incineration, and power generation industries.

Pyro-Putty® 950

  • Ceramic Fiber Filled, Organic-Resinous Gasket Seal
  • For sealing High Temperature Joints to 950 °F, 750 psi
  • Cures to a Tough, Pliable, Chemically Resistant Material
Typical Applications:
  • Turbines
  • Boilers
  • Heat Exchangers
  • Compressors
  • Pumps
  • Blowers
  • Piping
  • Ducting
  • Furnaces
  • Ovens
  • Steam Valves
  • Foundry Molds

Vendors: Aremco’s Pyro-Putty high temperature ceramic-metallic pastes seal joints and repair defects in cast aluminum, cast iron, steel and stainless steel to 2300°F (1260°C). Visit us today at Aremco.com or call 1 (845) 268-0039 to speak with an engineer.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.09 g/cc
Storage Temperature 40.0 - 90.0 °F
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 950 °F
 
Processing PropertiesOriginal ValueComments
Cure Time 1.00 hour
@Temperature 204 °C
 6.00 hour
@Temperature 107 °C
Shelf Life 6.00 Month
 
Descriptive Properties
ColorSilver Gray
FillerCeramic Fiber

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Aremco Ceramabond™ 571 High Temperature Ceramic Adhesive/Paste, Magnesium Oxide Filled
Silicon Carbide, Alpha SiC
COI Ceramics Nicalon™ CG SiCO Ceramic Fiber
3M Nextel™ 312 Industrial Ceramic Fiber
Aremco Pyro-Putty™ 2500 High Temperature Ceramic-Metallic Putty, Iron Oxide Filled

CAREM32 / 573

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.