MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
H.C. Starck Grade A 01 Boron Nitride, BN
Categories: Ceramic; Nitride

Material Notes: White powder.
  • Solid lubricant for high-temperature applications
  • Mold release for die casting and injection molding
  • Raw material for cubic BN
  • Thermally conductive filler for polymers
  • Composite ceramics, e.g. evaporation boats
  • Starting material for hot-pressed BN parts
  • Refractories

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Surface Area 4.0 - 7.5 m²/gBET
 
Component Elements PropertiesOriginal ValueComments
B2O3 <= 0.15 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Boron Nitride, BN
AISI Type O1 Oil-hardening Tool Steel, oil quenched at 800°C, tempered at 425°C
AISI 1060 Steel, as rolled
Boron Nitride, Cubic BN, (Borazone)
Momentive Performance Materials HBT Hot-Pressed Boron Nitride

CHCSTA034 / 1212

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.