MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
ExxonMobil LLDPE LL 6101RQ Linear Low Density Polyethylene Resin
Categories: Polymer; Thermoplastic; Polyethylene (PE); Linear Low Density (LLDPE)

Material Notes: Product Description: LL 6101 series are medium flow LLDPE grades, which offer excellent stiffness, heat distortion resistance and good environmental stress crack resistance. The excellent toughness and ESCR make LL 6101 grades an excellent blend partner for HDPE, where it can enhance the ESCR of items like buckets and lids.

Availability: Africa & Middle East, Asia Pacific and Europe

Additive:

  • Thermal Stabilizer: Yes
Applications:
  • Bottle Caps
  • Compounding (RQ version)
  • Containers
  • Door Mats
  • Dust Bins
  • Large Part Housewares
  • Lids

Information provided by ExxonMobil

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.924 g/ccExxonMobil method
ESCR 10% Igepal® 40 hour
@Temperature 50.0 °C
ASTM D1693B
Melt Flow 20 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 1500 psiASTM D638
Elongation at Break 100 %ASTM D638
Elongation at Yield 20 %ASTM D638
Flexural Modulus, 1% Secant 38000 psiASTM D790
Izod Impact, Notched (ISO) 22.0 ft-lb/in²ISO 180/1A
 
Thermal PropertiesOriginal ValueComments
Melting Point <= 253 °FPeak Melting Point; ExxonMobil method

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
ExxonMobil Escorene® LL-6101 LLDPE, Injection Grade
Overview of materials for High Density Polyethylene (HDPE), Rotational Molding Grade
Overview of materials for Low Density Polyethylene (LDPE), Molded
Overview of materials for Medium Density Polyethylene (MDPE), Rotational Molded
ExxonMobil LLDPE LL 6101XR Linear Low Density Polyethylene Resin (European Grade)

PEX99189 / 175425

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.