MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Metal adhesives

(Viewing data as-entered. Click here to return)
Tra-Con Tra-Bond 2151 Thermally Conductive Electrically Insulating Compound
Categories: Polymer; Adhesive; Thermoset; Epoxy

Material Notes: TRA-BOND 2151 is a thixotropic (smooth paste) heat conductive epoxy system that passes the NASA Outgassing Specification. It is used for staking transistors, diodes, resistors, integrated circuits and other heat-sensitive components to printed circuit boards. This two-part adhesive develops strong, durable, high-impact bonds at room temperature which improve heat transfer while maintaining electrical insulation. TRA-BOND 2151 bonds readily to itself, and to metals, silica, steatite, alumina, sapphire and other ceramics, glass, plastics and many other materials, because its coeffcient of thermal expansion provides a good match for those materials over a fairly wide temperature range. Fully cured TRA-BOND 2151 provides excellent resistance to salt solutions, mild acids and alkalis, and many other chemicals including petroleum solvents, lubricating oils, and alcohol. This adhesive complies with the requirements of NASA Outgassing Specification.

Information provided by Tra-Con Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 2.30 g/ccMixed
Solids Content 100 %Reactive Solids Content
Viscosity 40000 cP
@Temperature 25.0 °C
Mixed (rv #7, 10 rpm)
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 90
Tensile Strength, Yield 7500 psi30 min @ 65°C
Adhesive Bond Strength 880 psiLap shear, gold to gold, 4 hrs @ 65°C
 2150 psiLap shear, alum to alum, 24 hrs @ 25°C
 2850 psiLap shear, alum to alum, 2 hrs @ 65°C
Izod Impact, Notched 0.490 ft-lb/in
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 2.10e+15 ohm-cm
 3.20e+13 ohm-cm
@Temperature 75.0 °C
 
Thermal PropertiesOriginal ValueComments
CTE, linear 26.0 µm/m-°C
@Temperature 20.0 °C
Thermal Conductivity 0.950 W/m-K
Maximum Service Temperature, Air 115 °C
Minimum Service Temperature, Air -70.0 °C
Glass Transition Temp, Tg 60.0 °CUltimate Tg
 
Processing PropertiesOriginal ValueComments
Cure Time 2.00 - 4.00 hour
@Temperature 65.0 °C
 24.0 hour
@Temperature 25.0 °C
Pot Life 35 min100 grams
 45 min25 grams
Working Life 1.25 hour100 grams
 
Descriptive Properties
Color Blue
Mix Ratio, parts by weight100/9.5Resin/Hardener
Outgassing, NASA Passes
Thixotropic Index 1.75 rpm/50 rpm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Tra-Con Tra-Bond 2151T Thermally Conductive Electrically Insulating Compound
Tra-Con Tra-Bond 2156 Heat Conductive Electrically Insulating Compound
Tra-Con Tra-Bond 2159 Heat Conductive Electrically Insulating Compound
Tra-Con Tra-Bond 2152 Thermally Conductive Electrically Insulating Compound
Tra-Con Tra-Bond 2153 Thermally Conductive Electrically Insulating Compound

PTRAC032 / 70960

Metal adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.