MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
E-Polymers EFLEX® I2020 Ionomer
Categories: Polymer; Thermoplastic; Ionomer

Material Notes: I-series (Ionomer): E-FLEX Ionomer is a family of ethylene acrylic acid (E/AA) copolymers, in which part of the acrylic acid is neutralized with metal ions such as zinc (Zn) or sodium (Na) or magnesium (Mg). E-FLEX Ionomer resins deliver impact toughness, abrasion resistance and chemical resistance in a variety of consumer and industrial products. E-FLEX Ionomer can be used in packaging, molded consumer goods, sports goods, and polymer modification.

Information Provided by E-Polymers Co., Ltd.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.950 g/ccASTM D792
Melt Flow 0.80 g/10 minASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 60ASTM D2240
Tensile Strength 33.94 MPaASTM D882
Elongation at Break 370 %ASTM D882
 
Descriptive Properties
Metal CationNa

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
A. Schulman FORMION™ FI 120E Non-Reinforced, Extrusion Grade Zinc Ionomer
ExxonMobil Iotek® 7510 Zinc Ionomer Molding/Extrusion Resin
ExxonMobil Iotek® 8000 Sodium Ionomer Molding/Extrusion Resin
ExxonMobil Iotek® 8020 Sodium Ionomer Molding/Extrusion Resin
A. Schulman FORMION™ FI 234 20% Mineral Reinforced Ionomer / Nylon Alloy

PEPOLZ113 / 103610

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.