MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Metal adhesives

(Viewing data as-entered. Click here to return)
Master Bond EP21D3F2 Two component, high viscosity epoxy system for bonding, sealing and coating
Categories: Polymer; Thermoset; Epoxy; Epoxy Adhesive

Material Notes: Key Features:
  • Convenient handling
  • Excellent physical strength properties
  • Dimensionally stable
  • Opaque, light white color
Master Bond EP21D3F2 is a high viscosity, two component epoxy system for high performance bonding, sealing and coating. It is formulated to cure at room temperature or more rapidly at elevated temperatures. The optimum cure schedule is overnight at room temperature followed by 1-2 hours at 135-165°F. Its mix ratio is a non-critical four to one by weight. It has exceptionally low linear shrinkage upon cure, less than 0.1%. This system is 100% reactive and does not contain any solvents or diluents. EP21D3F2 has a superior profile of physical strength properties, notably its tensile modulus. It bonds well to a wide variety of materials including metals, composites, glass, ceramics, rubbers and many plastics. It is a reliable electrical insulator. The service temperature range is -80°F to +250°F. It has good chemical resistance to water, oils and fuels. A special feature of EP21D3F2 is its opaque, light white color and its high optical opacity. This versatile system should be considered in optical applications where the properties described above are required.

Product Advantages:

  • Easy to use
  • High viscosity and flowable
  • Good physical strength properties after curing
  • Special light white coloring with optical opacity

Information provided by Master Bond Inc.

Vendors: Master Bond is a leading manufacturer of adhesives, sealants, coatings and potting compounds. Master Bond’s vast product line consists of over 3,000 epoxy, polyurethane, silicone, cyanoacrylate and latex adhesives that vary in viscosity, cure speed, strength, chemical resistance, electrical properties, etc. Our custom adhesives offer design flexibility and provide excellent bonding performance. Visit www.masterbond.com.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.14 g/ccPart B
 1.23 g/ccPart A
Viscosity 20000 - 40000 cPPart A
 25000 - 75000 cPMixed
 20000 - 100000 cPPart B, thixotropic
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 80 - 90
Tensile Strength 7000 - 8000 psi
Tensile Modulus 450000 - 500000 psi
Adhesive Bond Strength 1000 - 1200 psiTensile Lap Shear; Al/Al
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity >= 1.00e+15 ohm-cm
Dielectric Constant 3.8
Dielectric Strength 450 V/mil
@Thickness 3.17 mm
 
Thermal PropertiesOriginal ValueComments
CTE, linear 45.0 - 50.0 µm/m-°C
Maximum Service Temperature, Air 121 °C
Minimum Service Temperature, Air -62.0 °C
 
Processing PropertiesOriginal ValueComments
Cure Time 1.00 - 2.00 hour
@Temperature 57.2 - 73.9 °C
Optimum cure schedule: overnight at 75°F plus 1-2 hours at 135-165°F
 2.00 - 3.00 hour
@Temperature 65.6 - 93.3 °C
Option 2
 24.0 - 48.0 hour
@Temperature 23.9 °C
Option 1
Working Life 30.0 - 40.0 min
@Temperature 23.9 °C
After mixing, 100 gram batch
Shelf Life 12.0 Month
 
Descriptive Properties
Mixing ratio4:1 by weight

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PMASTM602 / 248998

Metal adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.