MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

EVALCA EVAL® EF-E Ethylene Vinyl Alcohol Copolymer Film  (discontinued **)
Categories: Polymer; Film; Thermoplastic; Ethylene Vinyl Alcohol (EVOH)

Material Notes: 44 mol % Ethylene. Non oriented type film; property values for 20 µm film.

Data provided by EVALCA. Applications: EVOH is used in packaging applications because of its outstanding gas barrier properties.

EVAL™ is now produced as a part of the Kuraray product line.

Key Words: Ethylene Vinylalcohol
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Moisture Absorption at Equilibrium 2.5 %2.5 %65% RH
 2.5 %2.5 %65% RH
 5.0 %5.0 %100% RH
Moisture Vapor Transmission 0.720 cc-mm/m²-24hr-atm1.83 cc-mil/100 in²-24hr-atm40°C, 90% RH
Oxygen Transmission 0.0300 cc-mm/m²-24hr-atm0.0762 cc-mil/100 in²-24hr-atm20°C; 65% RH; Permeability increases significantly at higher moisture content.
Thickness 15.2 microns0.600 mil
 
Mechanical PropertiesMetricEnglishComments
Film Elongation at Break, MD 260 %260 %10%/min.; ASTM D638
Film Elongation at Break, TD 190 %190 %10%/min.; ASTM D638
Secant Modulus, MD 2.00 GPa290 ksiYoungs Modulus, ASTM D638, 10%/min.
Secant Modulus, TD 1.90 GPa276 ksiYoungs Modulus, ASTM D638, 10%/min.
Elmendorf Tear Strength MD 460 g460 gASTM D638
Elmendorf Tear Strength TD 440 g440 gASTM D638
Elmendorf Tear Strength, MD 30.2 g/micron767 g/mil0.6 mil; ASTM D638
Elmendorf Tear Strength, TD 28.9 g/micron733 g/mil0.6 mil; ASTM D638
Film Tensile Strength at Break, MD 70.0 MPa10200 psi10%/min.; ASTM D638
Film Tensile Strength at Break, TD 44.0 MPa6380 psi10%/min.; ASTM D638
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 1.20e+13 ohm-cm1.20e+13 ohm-cm
Surface Resistance 2.10e+15 ohm2.10e+15 ohm
Dielectric Constant 5.55.5Frequency Not Specified
Dissipation Factor 0.220.22Frequency Not Specified
 
Thermal PropertiesMetricEnglishComments
CTE, linear  80.0 µm/m-°C
@Temperature 20.0 °C
44.4 µin/in-°F
@Temperature 68.0 °F
Estimated by MatWeb from similar grades
 130 µm/m-°C
@Temperature 100 °C
72.2 µin/in-°F
@Temperature 212 °F
Estimated by MatWeb from similar grades
Specific Heat Capacity 2.40 J/g-°C0.574 BTU/lb-°FEstimated by MatWeb from similar grades
Thermal Conductivity 0.340 W/m-K2.36 BTU-in/hr-ft²-°FFor EVAL F101
Melting Point 164 °C327 °FDSC
 
Optical PropertiesMetricEnglishComments
Haze 1.7 %1.7 %65% RH
Gloss 90 %90 %65% RH

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
DuPont Selar® RB 421 EVOH Barrier Resin
Soarus SoarnoL® AT4403 Ethylene Vinyl Alcohol Copolymer
Soarus SoarnoL® DC3203F Ethylene Vinyl Alcohol Copolymer
Soarus SoarnoL® ET3808 Ethylene Vinyl Alcohol Copolymer
Overview of materials for Ethylene Vinyl Alcohol (EVOH)

PEVALE / 37304

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.