MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), 30% Glass Fiber Filled
Categories: Polymer; Thermoplastic; ABS Polymer; Acrylonitrile Butadiene Styrene (ABS), 30% Glass Fiber Filled

Material Notes: This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), 30% Glass Fiber Filled". Specific grades with glass content between 25% and 34% are included. Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 1.17 - 1.50 g/ccAverage value: 1.28 g/cc Grade Count:75
Filler Content 25.0 - 33.0 %Average value: 29.5 % Grade Count:12
Water Absorption 0.120 - 7.00 %Average value: 0.572 % Grade Count:16
Maximum Moisture Content 0.0200 - 0.150Average value: 0.0520 Grade Count:5
Linear Mold Shrinkage 0.00100 - 0.0250 cm/cmAverage value: 0.00215 cm/cm Grade Count:60
Linear Mold Shrinkage, Transverse 0.00100 - 0.0250 cm/cmAverage value: 0.00762 cm/cm Grade Count:4
Melt Flow 0.100 - 42.0 g/10 minAverage value: 5.63 g/10 min Grade Count:42
Ash 25.0 - 31.0 %Average value: 29.5 % Grade Count:8
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 88.0 - 125Average value: 111 Grade Count:29
Tensile Strength, Ultimate 39.0 - 120 MPaAverage value: 86.5 MPa Grade Count:49
Tensile Strength, Yield 51.7 - 117 MPaAverage value: 85.2 MPa Grade Count:40
Elongation at Break 1.00 - 6.00 %Average value: 2.45 % Grade Count:52
Elongation at Yield 1.00 - 6.00 %Average value: 2.83 % Grade Count:12
Modulus of Elasticity 3.30 - 10.0 GPaAverage value: 7.06 GPa Grade Count:27
Flexural Yield Strength 12.8 - 185 MPaAverage value: 122 MPa Grade Count:65
Flexural Modulus 0.687 - 10.0 GPaAverage value: 7.03 GPa Grade Count:70
Izod Impact, Notched 0.400 - 1.23 J/cmAverage value: 0.678 J/cm Grade Count:60
 0.600 - 0.600 J/cm
@Temperature 0.000 - 0.000 °C
Average value: 0.600 J/cm Grade Count:1
Izod Impact, Unnotched 2.14 - 4.81 J/cmAverage value: 3.15 J/cm Grade Count:21
Izod Impact, Notched (ISO) 4.00 - 6.00 kJ/m²Average value: 5.06 kJ/m² Grade Count:10
Charpy Impact Unnotched 1.30 - 7.00 J/cm²Average value: 3.43 J/cm² Grade Count:3
Charpy Impact, Notched 0.450 - 1.80 J/cm²Average value: 0.835 J/cm² Grade Count:10
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 1.00e+9 - 1.00e+16 ohm-cmAverage value: 5.02e+15 ohm-cm Grade Count:17
Surface Resistance 1.00e+10 - 1.00e+14 ohmAverage value: 6.02e+13 ohm Grade Count:5
Dielectric Strength 15.7 - 26.0 kV/mmAverage value: 18.5 kV/mm Grade Count:10
Arc Resistance 60.0 - 120 secAverage value: 81.7 sec Grade Count:3
 
Thermal PropertiesOriginal ValueComments
CTE, linear 17.0 - 30.6 µm/m-°CAverage value: 27.8 µm/m-°C Grade Count:12
Melting Point 165 - 225 °CAverage value: 203 °C Grade Count:3
Deflection Temperature at 0.46 MPa (66 psi) 96.7 - 200 °CAverage value: 110 °C Grade Count:37
Deflection Temperature at 1.8 MPa (264 psi) 83.0 - 180 °CAverage value: 103 °C Grade Count:63
Vicat Softening Point 93.0 - 205 °CAverage value: 115 °C Grade Count:15
Flammability, UL94 HB - 5VAGrade Count:36
 
Processing PropertiesOriginal ValueComments
Processing Temperature 180 - 260 °CAverage value: 215 °C Grade Count:10
Nozzle Temperature 200 - 274 °CAverage value: 234 °C Grade Count:13
Melt Temperature 160 - 288 °CAverage value: 226 °C Grade Count:29
Mold Temperature 20.0 - 100 °CAverage value: 67.0 °C Grade Count:38
Drying Temperature 70.0 - 100 °CAverage value: 82.9 °C Grade Count:31
Moisture Content 0.0100 - 0.100 %Average value: 0.0786 % Grade Count:7
Dew Point -17.8 °CAverage value: -17.8 °C Grade Count:3
Injection Pressure 4.83 - 103 MPaAverage value: 64.1 MPa Grade Count:14

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Molded
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), 10% Glass Fiber Filled
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), 20% Glass Fiber Filled
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), 30% Carbon Fiber Filled
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Heat Resistant, Molded

O1113 / 77803

Elmet Technologies

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.