MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
BIW Liquid Silicone Rubber, Oil-Resistant Grades
Categories: Polymer; Thermoset; Silicone; Silicone Rubber; Liquid Silicone Rubber (LSR)

Material Notes: BIW produces molded parts with a range of adjustable properties from this two-component LSR system. No individual grade can fit all properties within the reported ranges.

Information provided by BIW Isolierstoffe GmbH.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.29 - 1.34 g/ccDIN 53479 A
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 50 - 70DIN 53505
Tensile Strength 6.00 - 7.00 MPaDIN 53504
Elongation at Break 230 - 430 %DIN 53504
Resilience 55 - 60Rebound; DIN 53512
Tear Strength 15.0 - 18.0 kN/mASTM D624 B
Compression Set 17 - 25 %
@Temperature 175 °C,
Time 79200 sec
DIN 53517
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 1.00e+15 ohm-cmVDE 0303
Dielectric Strength 23.0 kV/mmVDE 0303
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 180 °CAll Colors
 280 °CBlack

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Momentive Performance Materials Silopren™ LSR 2620 Liquid Silicone Rubber - Fast Cure / High Tear
Momentive Performance Materials Silopren™ LSR 2610 Liquid Silicone Rubber - Fast Cure / High Tear
Momentive Performance Materials Silopren™ LSR 2020 Liquid Silicone Rubber - General Purpose
Momentive Performance Materials Silopren™ LSR 2003 Liquid Silicone Rubber - General Purpose
Elkem (Bluestar Silicones) SILBIONE® LSR 4301 Liquid Silicone Rubber

PBIWS982 / 192649

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.