MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

BP Amoco Accpro® 9433 Enhanced Polypropylene  (discontinued **)
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene, Molded

Material Notes: Suggested fabrication methods: Injection molding

Features: High stiffness, Surface hardness, Stain resistance, Antistatic, Nucleated

Complies with FDA specification, Title 21, CFR 177.1520.

Typical applications: Microwavable containers

Typical property data below from injection molded samples.

Key Words: High Stiffness, Surface hardness, Stain Resistance, Antistatic, Nucleated
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.886 - 0.926 g/cc0.0320 - 0.0335 lb/in³ASTM D1505
Water Absorption <= 0.010 %<= 0.010 %24 hours; ASTM D570
Linear Mold Shrinkage 0.010 - 0.025 cm/cm0.010 - 0.025 in/inASTM D955
Melt Flow 12 g/10 min
@Load 2.16 kg,
Temperature 230 °C
12 g/10 min
@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 109109ASTM D785
Tensile Strength, Yield 42.0 MPa6090 psiASTM D638
Elongation at Break 10 %10 %ASTM D638
Flexural Modulus 2.41 GPa350 ksiASTM D790A
Izod Impact, Notched 0.210 J/cm
@Diameter 3.17 mm
0.393 ft-lb/in
@Diameter 0.125 in
bar; ASTM D256
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 132 °C270 °FASTM D648
 
Compliance PropertiesMetricEnglishComments
FDA YesYes

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
BP Amoco ACCPRO® 9644X Injection Grade Polypropylene
Bamberger Polymers Bapolene® 4072NA Polypropylene
BP Amoco Accpro® 9934 Enhanced Polypropylene
Asahi Kasei Xyron™ X404H PPE/PS, High Stiffness, Ultra Low Warp Chassis
Bamberger Polymers Bapolene® 4062 Polypropylene, Injection Grade

PBPP09 / 27650

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.