MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Geon® Performance Solutions 92052 Exterior Extrusion PVC  (discontinued **)
Categories: Polymer; Thermoplastic; Vinyl (PVC); PVC, Extruded

Material Notes: Data provided by PolyOne.

Geon Performance Solutions was created from PolyOne in 2019.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.28 g/ccVaries with color; ASTM D792
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 77ASTM D2240
Tensile Strength, Ultimate 46.0 MPaat 5 cm/min. ASTM D638
Modulus of Elasticity 2.745 GPaat 5 cm/min. ASTM D638
Flexural Yield Strength 82.0 MPaASTM D790
Flexural Modulus 2.834 GPaASTM D790
Izod Impact, Notched 0.900 J/cm
@Diameter 3.20 mm
bar; ASTM D256
 
Thermal PropertiesOriginal ValueComments
CTE, linear 69.5 µm/m-°C
@Temperature 20.0 °C
ASTM D696
Deflection Temperature at 1.8 MPa (264 psi) 79.0 °CUnannealed; 6.4 cm (2.5 in.) bars; ASTM D648
 
Processing PropertiesOriginal ValueComments
Melt Temperature 196 - 199 °CExtrusion

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Versalis KOBLEND PCA PD 935 G2 PC+ABS, 10% Glass Fiber
Geon® Performance Solutions 91025 Interior Extrusion PVC
Geon® Performance Solutions 87020 Exterior Extrusion PVC
Avient Edgetek® CY-20GF/000 UV FR V0 PC/ABS Blend, Glass Filled
Geon® Performance Solutions 83530 Fiberloc PVC; 30% Glass Fiber Reinforced

PVIGG9 / 71904

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.