MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
KEP Kepital® F20-52 Acetal Copolymer
Categories: Polymer; Thermoplastic; Acetal (Polyoxymethylene, POM); Acetal Copolymer, Unreinforced

Material Notes: Information provided by US distributor Polymer Technology and Services, LLC (PTS).

Key Words: Polyacetal; Polyoxymethylene; Korea Engineering Plastics
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.41 g/ccASTM D792
Water Absorption 0.22 %24 hours at 73°F
Melt Flow 9.0 g/10 min
@Load 10.0 kg,
Temperature 220 °C
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell M 80ASTM D785
Tensile Strength, Yield 59.3 MPa
@Thickness 3.17 mm
Elongation at Break 50 %
@Thickness 3.17 mm
Flexural Yield Strength 85.5 MPa
@Thickness 3.17 mm
Flexural Modulus 2.55 GPa
@Thickness 3.17 mm
Izod Impact, Notched 0.530 J/cm
@Thickness 3.17 mm
 
Thermal PropertiesOriginal ValueComments
Melting Point 165 °CASTM D789
Deflection Temperature at 0.46 MPa (66 psi) 158 °CASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 110 °CASTM D648
 
Processing PropertiesOriginal ValueComments
Rear Barrel Temperature 329 - 356 °F
Middle Barrel Temperature 347 - 383 °F
Front Barrel Temperature 356 - 383 °F
Nozzle Temperature 356 - 383 °F
Melt Temperature 365 - 428 °F
Mold Temperature 158 - 194 °F
Drying Temperature 176 - 194 °F
Dry Time 3 - 4 hour
Injection Pressure 7000 - 17000 psi

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
KEP Kepital® F20 Acetal Copolymer
BASF Ultraform® H 2320 006 Q600 POM
Chi Mei Polylac® PA-737 ABS - High Flow
Chi Mei Polylac® PA-746 ABS - High Flow
Chi Mei Polylac® PA-746H ABS - High Flow

PLBK01 / 50371

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.