MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Chevron Phillips Marlex® HHM 5202 BN High Density Ethylene Hexene-1 Copolymer
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE); High Density Polyethylene (HDPE), Blow Molding Grade

Material Notes: High Density Ethylene Hexene-1 Copolymer

Customer Benefits: For the blow molder who wants to stock one resin that will be suitable for most of his customers' packaging needs. Lightweight containers have excellent environmental stress cracking resistance, good stiffness and impact strength. These same advantages will be obtained for Thermoformed parts.

Applications: Containers for bleach and detergents and chemicals. Molded or formed industrial housings, tanks, and shrouds.

Processing Recommendations:
Blow Molding Stock Temperature: Upper Limit: 204°C, Lower Limit: 171°C
Extrusion Melt Temperature: Upper Limit: 216°C, Lower Limit: 194°C
Thermoforming Surface Temperature: Upper Limit: 182°C, Lower Limit: 171°C

Specification Data: ASTM D4976 - PE 235. ASTM D1248 - Type III, Class A, Category 5. FDA Regulation 177.1520. Suitable for food packaging. Listed in Drug Master File

Sag Upper Limit: 23 cm, Lower Limit: 18 cm; 2 ft. X 4ft. X 125 mil thick blank heated to forming temperature.

Data provided by Chevron Phillips Chemical Company, LP.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.952 g/ccASTM D1505
ESCR 100% Igepal® 50 hourCondition A, F50 CO-630; ASTM D1693
ESCR, Bottle 250 hour
@Temperature 60.0 °C
F50
Melt Flow 0.35 g/10 minCondition 190/2.16; ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 27.0 MPa2 in per min; ASTM D638 Type IV
Elongation at Break >= 600 %2 in per min; ASTM D638 Type IV
Flexural Modulus 1.309 GPaASTM D790
 
Thermal PropertiesOriginal ValueComments
Brittleness Temperature <= -118 °CASTM D746
 
Processing PropertiesOriginal ValueComments
Processing Temperature 171 - 182 °CThermoforming Surface
 171 - 204 °CBlow Molding
 194 - 216 °CExtrusion

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Ineos B53-35H-124 Blow Molding Grade Polyethylene
Chevron Phillips Marlex® HHM 5502 LD High Density Ethylene Hexene Copolymer with Antistat
Chevron Phillips Marlex® 9509HF High Density Polyethylene, Blow Molding
Chevron Phillips Marlex® 9035 High Density Polyethylene, Injection Molding
Chevron Phillips Marlex® HHM 4903 High Density Ethylene Hexene Copolymer

PCHEVM18 / 20308

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.