MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
Lotte Advanced Materials Starex® SP-0180 ABS, Unreinforced Extrusion Grade
Categories: Polymer; Thermoplastic; ABS Polymer; Acrylonitrile Butadiene Styrene (ABS), Extruded

Material Notes:

Information provided by Samsung Cheil Industries.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.04 g/ccASTM D792
Melt Flow 6.0 g/10 min
@Load 10.0 kg,
Temperature 220 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 98ASTM D785
Tensile Strength, Yield 370 kg(f)/cm²5 mm/min; ASTM D638
Flexural Strength 53.9 MPa2.8 mm/min; ASTM D790
Flexural Modulus 19000 kg(f)/cm²2.8 mm/min; ASTM D790
Izod Impact, Notched 38.0 kg-cm/cm
@Thickness 6.35 mm
ASTM D256
 
Thermal PropertiesOriginal ValueComments
Vicat Softening Point 97.0 °CB/50; ISO R306

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Lotte Advanced Materials Starex® PT-0180 J ABS
Lotte Advanced Materials Starex® SD-0150 ABS, Unreinforced
Lotte Advanced Materials Starex® SP-0183 ABS, Unreinforced Extrusion Grade
Lotte Advanced Materials Starex® SP-0170 ABS, Unreinforced Extrusion Grade
Lotte Advanced Materials Starex® SV-0165 U ABS, Unreinforced Extrusion Grade

PSAMSU884 / 146701

Elmet Technologies

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.