MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Syensqo (Solvay Specialty Polymers) Polidan® T/A Polyethylene, Crosslinked (XLPE)
Categories: Polymer; Thermoplastic; Polyethylene (PE)

Material Notes: POLIDAN® T/A is a silane crosslinkable PE compound which is used together with a catalyst masterbatch to accelerate the crosslinking reaction. It is used for flexible crosslinkable pipes.

Applications

- POLIDAN® T/A is used for the production of pipes for domestic hot and cold water supply as well as indoor/outdoor gas distribution. This compound is designed for both mono layer and composite pipe solutions.

Crosslinkable; Good Processing Stability; High Density

Uses: Piping; Plumbing Parts; Potable Water Applications

Processing: Extrusion; Pipe Extrusion

Agency Ratings: DVGW W270; ISO 15875 /2; ISO 9080 PE 100; ISO/DIS 12162 - MRS 10 MPa, PE100; KTW Unspecified Rating; NSF STD-14; NSF STD-61

Availability: Africa & Middle East; Asia Pacific; Europe; Latin America

Information provided by Solvay Specialty Polymers.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.950 g/ccASTM D792
Melt Flow 0.50 g/10 min
@Load 5.00 kg,
Temperature 190 °C
ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength >= 20.0 MPaASTM D638
Elongation at Break >= 350 %ASTM D638
Tensile Modulus 1100 MPaISO 527-2
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 140 µm/m-°CASTM D696
Specific Heat Capacity 1.90 J/g-°C
@Temperature 23.0 °C
ASTM C351
Thermal Conductivity 0.470 - 0.490 W/m-KASTM C177
Vicat Softening Point 127 °CASTM D152
 
Processing PropertiesOriginal ValueComments
Zone 1 150 - 200 °C
Zone 2 150 - 200 °C
Zone 3 150 - 200 °C
Zone 4 150 - 200 °C
Zone 5 150 - 200 °C
Die Temperature 210 °C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Syensqo (Solvay Specialty Polymers) Polidan® EC/51 Polyethylene, Crosslinked (XLPE)
Avient Syncure™ System S112NA Polyethylene, Crosslinked (XLPE)
Syensqo (Solvay Specialty Polymers) Polidan® TUX 100 Polyethylene, Crosslinked (XLPE)
Syensqo (Solvay Specialty Polymers) Polidan® EC/110 Polyethylene, Crosslinked (XLPE)
Syensqo (Solvay Specialty Polymers) Polidan® PNT 0553/23 Polyethylene, Crosslinked (XLPE)

PSOL8Y6310 / 193231

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.