MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Michelman® Michem ® Flex B7010 Transparent oxygen barrier coating
Categories: Fluid; Polymer; Thermoplastic; Adhesives, Sealants, and Coatings

Material Notes: Transparent oxygen barrier coating for offline flexible packaging coating applications. Michem® Flex B7010 is designed to be applied offline to polymer materials using gravure or flexographic coating processes. Suggested coat weight is 0.3 dry gsm. At the recommended coating weight, the dried coating is transparent, non-blocking and contributes to oxygen barrier properties of polymer materials. It should be used undiluted and dried thoroughly after application. This product was specifically designed for and is available only in Asia. Usage: A transparent high oxygen barrier water-based coating designed primarily for offline applications of polymer materials. It is more durable and can withstand fracturing and pinholes compared to traditional barrier coatings. It can also be combined with metallization processes as a protective oxygen barrier coating. Applications (properties imparted): Functional Coatings (Substrate - film, oxygen barrier).

Handling: Handle in accordance with good industrial hygiene and safety practice. Use personal protective equipment as required.

Information provided by Michelman

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.990 - 1.01 g/cc0.990 - 1.01 g/cc
Solids Content 9.5 - 10.5 %9.5 - 10.5 %Non-Volatiles
pH 3.0 - 6.03.0 - 6.0
Brookfield Viscosity 0.00 - 100 cP0.00 - 100 cPSpindle #1. 60 RPM.
 
Processing PropertiesMetricEnglishComments
Shelf Life 12.0 Month12.0 MonthDry, cool and well-ventilated place
 
Descriptive Properties
AppearanceClear, yellow to brown liquid
Freeze/Thaw StabilityNone: protect from freezing

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

WMICHE9837 / 287432

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.