MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
BASF Ultramid® 8260 40% Mineral Filled PA6 (Dry)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, 40% Mineral Filled

Material Notes: Ultramid 8260 is a 40% mineral reinforced PA6 injection molding compound. It possesses high stiffness, dimensional stability and heat resistance combined with excellent processability including low warp and resistance to sink-mark formation. It is also available in heat stabilized (Ultramid 8260 HS) versions. It can be painted or chrome plated and is also available in pigmented versions.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.49 g/ccISO 1183
Melt Density 1.291 g/cc
@Temperature >=220 °C
ISO 1183
Water Absorption 1.1 %24 hour; ISO Test
 5.7 %ISO 62
Moisture Absorption at Equilibrium 1.6 %23°C/50% R.H.; ISO 62
Linear Mold Shrinkage 0.0090 cm/cmASTM Data; MD
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 119ASTM Test
Tensile Strength at Break 90.0 MPa0.2 in/min; ASTM Test
Tensile Strength, Ultimate 85.0 MPa5mm/min; ISO 527
Elongation at Break 10 %5mm/min; ISO 527
 10 %0.2 in/min; ASTM Test
Tensile Modulus 6400 MPa1mm/min; ISO 527
 970 MPa
@Temperature 120 °C
ISO Data
 1360 MPa
@Temperature 80.0 °C
ISO Data
 8310 MPa
@Temperature -40.0 °C
ISO Data
Flexural Strength 138 MPaASTM Test
 140 MPaISO Data
 34.0 MPa
@Temperature 120 °C
ASTM Test
 35.0 MPa
@Temperature 93.0 °C
ASTM Test
 55.0 MPa
@Temperature 65.0 °C
ASTM Test
 207 MPa
@Temperature -40.0 °C
ASTM Test
Flexural Modulus 5200 MPaISO Data
 5760 MPaASTM Test
 810 MPa
@Temperature 93.0 °C
ASTM Test
 815 MPa
@Temperature 120 °C
ASTM Test
 1540 MPa
@Temperature 65.0 °C
ASTM Test
Izod Impact, Notched 0.530 J/cm
@Thickness 3.17 mm
ASTM Test
Izod Impact, Unnotched 16.4 J/cmASTM Test
Charpy Impact Unnotched 11.5 J/cm²ISO 179
Charpy Impact, Notched 0.300 J/cm²ISO 179
 0.300 J/cm²
@Temperature -30.0 °C
ISO 179
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity >= 1.00e+13 ohm-cmIEC 60093
 
Thermal PropertiesOriginal ValueComments
CTE, linear 50.0 µm/m-°C
@Temperature -30.0 - 30.0 °C
ASTM Test
CTE, linear, Parallel to Flow 46.0 µm/m-°CISO 11359
CTE, linear, Transverse to Flow 58.0 µm/m-°CISO 11359
Specific Heat Capacity 1.999 J/g-°CMelt
Thermal Conductivity 0.281 W/m-KMelt
Melting Point 220 °C10 K/min
 220 °CASTM Test
Deflection Temperature at 0.46 MPa (66 psi) 195 °CISO 75
Deflection Temperature at 1.8 MPa (264 psi) 125 °CASTM Test
 
Processing PropertiesOriginal ValueComments
Melt Temperature 275 °CInjection molding
Mold Temperature 95.0 °CInjection molding
 
Descriptive Properties
ColorNatural
Commercial StatusActive America
FormPellets
Impact ModifiedNo
Primary Processing TechniqueInjection Molding
ProcessingInjection Molding
Special characteristicX

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
BASF Ultramid® A3EG3 15% Glass Filled PA66 (Dry)
BASF Ultramid® 8260 40% Mineral Filled PA6 (Conditioned)
BASF Ultramid® 8260 HS BK-102 40% Mineral Filled PA6 (Dry)
BASF Ultramid® 8266G HS BK-102 15/25% Glass/Mineral Filled PA6 (Dry)
Celanese Minlon® 73M40 NC010 PA6-MD40

PBASF9181 / 84945

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.