MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
ExxonMobil Escorene® UL 7510 Adhesive Application Resin  (discontinued **)
Categories: Polymer; Adhesive; Thermoplastic; Ethylene Vinyl Acetate; Ethylene Vinyl Acetate Copolymer (EVA), Adhesive/Sealant Grade

Material Notes: Escorene Ultra UL 7510 is a very high flow, 18.7% vinyl acetate copolymer that has very good compatibility with hydrocarbon tackifiers and most waxes. It is suitable for making hot melt adhesives, sealants and wax blends.

Availability: Asia Pacific, Latin America, North America and South America

Additive:

  • Antiblock: No
  • Slip: No
  • Thermal Stabilizer: Yes
Applications:
  • Adhesives and Sealants
  • Hot Melt Adhesives
  • Industrial Sealants
  • Wax Blends
Information provided by ExxonMobil Chemical

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.933 g/ccExxonMobil Method
Vinyl Acetate Content 18.7 %ExxonMobil Method
Melt Flow 500 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 7515s; ASTM D2240
Hardness, Shore D 2315s; ASTM D2240
Tensile Strength at Break 420 psiASTM D638
Elongation at Break 330 %ASTM D638
Flexural Modulus, 1% Secant 5400 psiASTM D790
 
Thermal PropertiesOriginal ValueComments
Melting Point 172 °FPeak Melting Temperature; ExxonMobil Method

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Arkema EVATANE® 20-20 Copolymer Ethylene - Vinyl Acetate
ExxonMobil Escorene® UL 7520 Adhesive Application Resin
ExxonMobil Escorene® UL 8705 Adhesive Application Resin
ExxonMobil Escorene® UL-7505 EVA Copolymer, Adhesive and Sealant Grade
Overview of materials for Silicone, RTV, Adhesive/Sealant Grade

PEXB159 / 37464

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.