MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Covestro Makrolon® AR sheet Polycarbonate
Categories: Polymer; Thermoplastic; Polycarbonate (PC)

Material Notes: Abrasion resistant Makrolon® AR sheet is a one or both sides hard-coated polycarbonate product that adds higher abrasion resistance and surface hardness to polycarbonate’s inherent performance benefits of impact strength and clarity. The proprietary hard-coat also provides chemical resistance and long lasting outdoor weathering performance. This product is available in clear, a range of standard tints, or can be custom matched to any color. Makrolon AR sheet has a seven (7) year Limited Product Warranty against breakage, yellowing, and hazing.

Applications: Flat architectural glazing, machine guards, and laminates

Information provided by Covestro

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.20 g/cc1.20 g/ccASTM D792
Water Absorption 0.15 %
@Time 86400 sec
0.15 %
@Time 24.0 hour
ASTM D570
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell M 7070ASTM D785
Hardness, Rockwell R 118118ASTM D785
Tensile Strength at Break 65.5 MPa9500 psiASTM D638
Tensile Strength, Yield 62.1 MPa9010 psiASTM D638
Elongation at Break 110 %110 %ASTM D638
Tensile Modulus 2.34 GPa339 ksiASTM D638
Flexural Strength 93.1 MPa13500 psiASTM D790
Flexural Modulus 2.38 GPa345 ksiASTM D790
Compressive Strength 86.2 MPa12500 psiASTM D695
Compressive Modulus 2.38 GPa345 ksiASTM D695
Poissons Ratio 0.380.38ASTM E132
Shear Modulus 0.786 GPa114 ksiASTM D732
Shear Strength 41.4 MPa6000 psiYield; ASTM D732
 68.9 MPa10000 psiBreak; ASTM D732
Izod Impact, Notched 8.54 J/cm
@Thickness 3.17 mm
16.0 ft-lb/in
@Thickness 0.125 in
ASTM D256
Izod Impact, Unnotched NB
@Thickness 3.17 mm
NB
@Thickness 0.125 in
ASTM D256
Impact Test >= 63.7 J
@Thickness 3.17 mm
>= 47.0 ft-lb
@Thickness 0.125 in
ASTM D3763
Taber Abrasion, mg/1000 Cycles 2.0
@Load 5.00 kg
2.0
@Load 11.0 lb
CS-10F Wheel; ASTM D1044
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 8.20e+16 ohm-cm8.20e+16 ohm-cmASTM D257
Dielectric Constant  2.96
@Frequency 10 Hz
2.96
@Frequency 10 Hz
ASTM D150
 3.17
@Frequency 60 Hz
3.17
@Frequency 60 Hz
ASTM D150
Dielectric Strength 15.0 kV/mm
@Thickness 0.125 mm
381 kV/in
@Thickness 0.00492 in
ASTM D149
Dissipation Factor 0.00090
@Frequency 60 Hz
0.00090
@Frequency 60 Hz
ASTM D150
Arc Resistance 10 sec10 secStinless Steel Strip
 120 sec120 sec
 
Thermal PropertiesMetricEnglishComments
CTE, linear 67.5 µm/m-°C37.5 µin/in-°FASTM D696
Thermal Conductivity 0.195 W/m-K1.35 BTU-in/hr-ft²-°FASTM C177
Deflection Temperature at 0.46 MPa (66 psi) 142 °C288 °FASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 132 °C270 °FASTM D648
Brittleness Temperature 93.3 °C200 °FASTM D746
 
Optical PropertiesMetricEnglishComments
Refractive Index 1.5861.586ASTM D542
Yellow Index 0.25 %0.25 %
 2.0 %2.0 %2.8 years
 3.0 %3.0 %6 years
Transmission, Visible  18 %
@Thickness 3.00 mm
18 %
@Thickness 0.118 in
I35 Dark Gray; ASTM D1003
 50 %
@Thickness 3.00 mm
50 %
@Thickness 0.118 in
I30 Gray; ASTM D1003
 50 %
@Thickness 3.00 mm
50 %
@Thickness 0.118 in
K09 Bronze; ASTM D1003
 86 %
@Thickness 3.00 mm
86 %
@Thickness 0.118 in
Clear; ASTM D1003
 
Descriptive Properties
Chemical ResistanceAcetone>24 Hrs
 Ammonia (10% concentration)>24 Hrs
 Antifreeze (50/50)>24 Hrs
 Benzene>24 Hrs
 Bleach (Clorox concentrated)>24 Hrs
 Chloroform>24 Hrs
 Denatured Alcohol>24 Hrs
 Di (2-ethylhexyl) phthalate>24 Hrs
 Diesel Oil>24 Hrs
 Hydrochloric Acid (20%)>24 Hrs
 Isopropyl Alcohol (IPA)>24 Hrs
 Kerosene>24 Hrs
 Methyl Alcohol>24 Hrs
 Methyl Butyl Ketone>24 Hrs
 Methyl Ethyl Ketone>24 Hrs
 Methylene Chloride>24 Hrs
 Naphthalene, 1-bromo->24 Hrs
 Nitric Acid (20%)>24 Hrs
 Potassium Hydroxide - Lye (10%)>24 Hrs
 Sodium Hydroxide (10%)>24 Hrs
 Sulfuric Acid (20%)>24 Hrs
 Toluene>24 Hrs
 Turpentine>24 Hrs
 Unleaded Gasoline (87 Octane)>24 Hrs
 Vinegar>24 Hrs
 Xylene>24 Hrs
Shading Coefficient0.77Gray or Bronze @ 0.236", NFRC 100-2010
 0.97Clear @ 0.236", NFRC 100-2010
U-value0.78 BTU/hr-ft2-°F0.375", summer, NFRC 100-2010
 0.85 BTU/hr-ft2-°F0.236", summer, NFRC 100-2010
 0.85 BTU/hr-ft2-°F0.375", winter, NFRC 100-2010
 0.92 BTU/hr-ft2-°F0.236", winter, NFRC 100-2010

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Covestro Makrolon® UV sheet Polycarbonate
Covestro Makrolon® FP sheet Polycarbonate
Covestro Makrolon® GP Matte sheet Polycarbonate
Covestro Makrolon® GP Pebble sheet Polycarbonate
Covestro Makrolon® GP Prismatic sheet Polycarbonate

PCOVEST0818 / 202601

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.